    • 56. 发明申请
    • Method for increasing the stability and/or load carrying ability of work pieces by means of friction welding
    • 通过摩擦焊接增加工件的稳定性和/或承载能力的方法
    • US20060266797A1
    • 2006-11-30
    • US10568321
    • 2004-07-14
    • Karl KainerNorbert HottHajo DieringaJorge SantosAxel Meyer
    • Karl KainerNorbert HottHajo DieringaJorge SantosAxel Meyer
    • A47J36/02
    • B23K20/12B23K2103/10F16B5/01F16B11/004F16B37/12F16B43/00
    • The invention relates to a method for at least locally increasing the stability and/or load carrying ability of work pieces (10), whereby first of all a first work piece (11) is produced by means of a conventional manufacturing method. The inventive method is characterized by the following steps: a) the first work piece (11) is then provided with a hole (13) in the area where stability and/or load carrying ability are to be increased; b) a second work piece (12) which consists of a stability-and/or load carrying ability-increasing material is introduced into the hole (13); c) in this state, the second work piece (12) is rubbed relative to the first work piece (11) according to the friction welding method until the welding temperature is reached which lies below the melting temperature of the two work pieces (11, 12), thereby obtaining a friction-welded connection between the first work piece (11) and the second work piece (12) and producing the work piece (10).
    • 本发明涉及一种用于至少局部增加工件(10)的稳定性和/或承载能力的方法,由此首先通过常规制造方法制造第一工件(11)。 本发明的方法的特征在于以下步骤:a)第一工件(11)在要增加稳定性和/或承载能力的区域中设置有孔(13) b)将由稳定性和/或负载能力增强材料组成的第二工件(12)引入孔(13)中; c)在这种状态下,第二工件(12)根据摩擦焊接方式相对于第一工件(11)摩擦直到达到低于两个工件(11,11)的熔化温度的焊接温度, 12),从而获得第一工件(11)和第二工件(12)之间的摩擦焊接连接并制造工件(10)。