    • 53. 发明专利
    • SILICON STEEL PLATE HAVING THERMOSTABLE, EXTREMELY LOW CORE LOSS, AND UNIDIRECTIONAL PROPERTIES
    • JPS63278209A
    • 1988-11-15
    • JP2400188
    • 1988-02-05
    • KAWASAKI STEEL CO
    • IGUCHI MASAOITO ISAO
    • C23C14/06C22C38/00H01F1/18
    • PURPOSE:To obtain a silicon steel plate having excellent thermostable and unidirectional properties without bring about the deterioration in the performance because of a high temperature treatment by forming a mixture phase among Fe atoms, accelarating ions, and evaporation inos between tension films on the polishing treatment surface of the silicon steel phate as a substrate. CONSTITUTION:A mixture phase with base steels is mainly formed with at least on kind of nitrides and/or carbides chosen out of the above nitrides and/or carbides of Ti, Zr, Hf, V, Nb, Ta, Mn, Cr, Mo, W, Co, Ni, Al, B, and Si at the surface of a unidirectional silicon steel plate where its finishing annealing is performed and non-metallic substances are removed or further at its flat surface finished by polishing and through the mixture phase with these base steels, tension films having a layer of 0.005-5 mum, at least are firmly deposited on the surface of the above steel plate and further, another tension film is deposited by putting it together with an insulation coating baking layer on the initial tension film. The film thickness of the tension films is adaptable within a range 0.005-5 mum. When it is less than 0.005 mum, it does not contribute toword necessary tension and on the other hand, when it exceeds 5 mum, space factor and adhesion decrease.
    • 57. 发明专利
    • GRAIN ORIENTED SILICON STEEL SHEET HAVING EXCELLENT MAGNETIC CHARACTERISTIC AND ITS PRODUCTION
    • JPS63130747A
    • 1988-06-02
    • JP27734886
    • 1986-11-20
    • KAWASAKI STEEL CO
    • KOHO HIROSHIITO ISAOIGUCHI MASAO
    • C23C14/06C21D8/12C22C38/00C22C38/12
    • PURPOSE:To improve both of a magnetic flux density and iron loss characteristic by effectively fining secondary recrystallization grains to improve the B10 value thereof and smoothing the surface of steel products and effectively utilizing a tension applied extremely thin film to improve the W17/50 value. CONSTITUTION:The linear strain which is along the transverse direction of a silicon steel sheet subjected to finish annealing and penetrates the sheet thickness is incorporated at 1-30% strain quantity into said steel sheet. The steel sheet is then subjected to gradient annealing under the conditions of >=700 deg.C and >=1 deg.C/cm temp. gradient across the transverse direction of the sheet; thereafter, the oxide on the surface of the steel sheet is removed and the surface is finished to a specular surface of =1 kinds of nitride and/or carbide of Ti, Nb, Si, etc., and oxide of Al, Si, Mn, etc., is formed by a vapor deposition method on such surface. The titled steel sheet having the linear recrystal region which extends in the transverse direction of the sheet by forming a grain boundary to the matrix, penetrates the sheet thickness, has >=1.0mm grain size and has within 10 deg. deviation of the axis in the rolling direction and having the above-mentioned extremely thin film is thereby obtd.