    • 56. 发明授权
    • Crosslinked polymer solutions and methods of use
    • 交联聚合物溶液及使用方法
    • US07888295B2
    • 2011-02-15
    • US11672829
    • 2007-02-08
    • Diankui FuAndrey Federov
    • Diankui FuAndrey Federov
    • C09K8/60C09K8/68C09K8/74
    • C09K8/685C09K8/70
    • A well treatment composition is formed from an aqueous crosslinkable hydrated polymer solution. Combined with the polymer solution is a solid boric acid or borate crosslinking agent and a solid metal oxide or metal hydroxide pH buffering agent that has limited solubility (less than 100 kg/m3 at 20° C.) within the polymer solution that provides the solution with a pH of from about 8 to about 11. The composition may be introduced into a subterranean formation through a wellbore that penetrates the formation. The composition may provide at least one of shortened shear recovery time and an increase in the thermal stability of the aqueous polymer solution.
    • 由水性可交联水合聚合物溶液形成良好的处理组合物。 与聚合物溶液结合是固体硼酸或硼酸盐交联剂和固体金属氧化物或金属氢氧化物pH缓冲剂,其在提供溶液的聚合物溶液中具有有限的溶解度(在20℃下小于100kg / m 3) 其pH值为约8至约11.组合物可以通过穿透地层的井筒引入地下地层。 组合物可以提供缩短的剪切恢复时间和聚合物水溶液的热稳定性的增加中的至少一种。
    • 59. 发明授权
    • Method of plugging fractured formation
    • 堵塞断层形成的方法
    • US07578346B2
    • 2009-08-25
    • US11557726
    • 2006-11-08
    • Diankui FuKreso Kurt Butula
    • Diankui FuKreso Kurt Butula
    • E21B43/267
    • E21B43/267C09K8/68C09K8/80C09K8/805
    • A material and method for treating a fractured formation penetrated by a wellbore includes providing a quantity of resin coated particles having a particle size of from about 0.2 mm to about 2.35 mm. A quantity of smaller deformable or non-deformable particles is combined with the resin coated particles to form a generally uniform consolidated particle pack when mixed together and subjected to at least one of heat and pressure. A slurry of the particles is formed with a carrier fluid capable of suspending the particles. The slurry of particles is introduced into the wellbore of the formation. The resin coated particles and smaller deformable particles thus may form a consolidated particle pack in at least a portion of the fractures of the formation.
    • 用于处理由井筒穿透的断裂地层的材料和方法包括提供一定量的具有约0.2mm至约2.35mm的粒度的树脂涂覆的颗粒。 一些较小的可变形或不可变形的颗粒与树脂涂覆的颗粒结合以在混合在一起并经受至少一种热和压力时形成大致均匀的固体颗粒组。 用能够悬浮颗粒的载体流体形成颗粒的浆料。 将颗粒的浆料引入地层的井眼。 因此,树脂涂覆的颗粒和较小的可变形颗粒可以在地层的至少一部分裂缝中形成固结的颗粒组。