会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 51. 发明授权
    • Magnetic recording medium and process for producing the same
    • 磁记录介质及其制造方法
    • US06221519B1
    • 2001-04-24
    • US09272622
    • 1999-03-19
    • Takanori DoiKousaku TamariYasuo KakiharaKenichi NakataMitsuru MatsuuraSetsuo Yamamoto
    • Takanori DoiKousaku TamariYasuo KakiharaKenichi NakataMitsuru MatsuuraSetsuo Yamamoto
    • G11B566
    • G11B5/7325G11B5/656G11B5/84G11B5/8404Y10S428/90
    • A magnetic recording medium comprising: a plastic substrate; a nickel oxide underlayer formed on said substrate; and a cobalt-containing maghemite thin film formed on said nickel oxide underlayer, containing cobalt at a molar ratio of cobalt to iron of 0.01:1 to 0.1:1, and having either a spacing of a plane (311) of not more than 2.510 Å, a spacing of a plane (222) of not more than 2.415 Å or a spacing of a plane (220) of not more than 2.950 Å, a ratio value of an X-ray diffraction pattern peak intensity of either of the planes (311), (222) and (220) of said cobalt-containing maghemite thin film to an X-ray diffraction pattern peak intensity of the plane (400) thereof being more than 0.5. Such magnetic recording medium suitably applicable to existent magnetic recording systems using a ring-type magnetic head and capable of using a plastic substrate for providing a magnetic recording medium for high-density recording.
    • 一种磁记录介质,包括:塑料基板;形成在所述基板上的氧化镍底层; 和在所述氧化镍底层上形成的含钴的磁赤铁矿薄膜,其含有钴与铁的摩尔比为0.01:1至0.1:1的钴,并且具有不大于2.510的平面(311)的间隔 ,平面(222)的间距不大于2.415或平面(220)的间距不大于2.950,任一平面(311)的X射线衍射图峰值强度的比值 ),所述含钴磁赤铁矿薄膜的(222)和(220)相对于所述平面(400)的X射线衍射图峰值强度大于0.5。 这种磁记录介质适用于使用环形磁头的现有磁记录系统,并能够使用塑料基板提供用于高密度记录的磁记录介质。