    • PULTRUSION OF POLY-4-HYDROXYBUTYRATE AND COPOLYMERS THEREOF
    • 聚合物聚合-4-羟基丁酸酯共聚物
    • EP3062995A1
    • 2016-09-07
    • EP14803273.3
    • 2014-10-31
    • Tepha, Inc.
    • GANATRA, AmitSHAH, BhavinRIZK, SaidMARTIN, David, P.WILLIAMS, Simon, F.
    • B29C70/52A61L27/14A61L27/40A61L31/04A61L27/18A61L31/06C08L67/04
    • A61L27/18A61L27/26A61L31/041A61L31/06B29C70/52C08G63/06C08L67/04
    • Compositions of P4HB (poly-4-hydroxybutyrate) and copolymers thereof, have been developed for pultrusion, as well as processes to produce profiles from these compositions by pultrusion. These pultrusion processes provide profiles without causing structural damage to the surface of the profile. The profiles may be used in medical applications. These compositions include P4HB, and copolymers thereof, having intrinsic viscosities less than 3.2 dl/g but greater than 0.8 dl/g. The profile may be formed using conditions such as: pull rate of 0.1 to 100 mm/min, die temperature of up to 95°C, rod stock temperature up to 95°C, draw ratio of up to 100X, pulling force of greater than 10 MPa, and clamping pressure at least 10 % higher than the pulling force. Preferably, the profile is formed by pulling the rod stock through a series of dies placed at intervals with the hole sizes decreasing in diameter by 0.1 to 10 mm.
    • P4HB(聚-4-羟基丁酸酯)及其共聚物的组合物已被开发用于拉挤成型,以及通过拉挤成型从这些组合物生产型材的方法。 这些拉挤成型工艺提供型材,而不会对轮廓的表面造成结构损坏。 型材可用于医疗应用。 这些组合物包括其特性粘度小于3.2dl / g但大于0.8dl / g的P4HB及其共聚物。 外形可以采用以下条件形成:拉伸速度为0.1〜100mm / min,模具温度可达95℃,棒料温度可达95℃,拉伸比可达100×,拉力 大于10MPa,并且夹紧压力比拉力高至少10%。 优选地,通过将​​棒材拉伸通过一系列模具而形成,所述一系列模具以直径减小0.1至10mm的孔的间隔间隔放置。