    • 32. 发明授权
    • Method of making wet process panels of composite wood material with
semi-matching contoured pressure plates
    • 用半匹配成型压板制作复合木材的湿法面板的方法
    • US4726881A
    • 1988-02-23
    • US730241
    • 1985-05-02
    • William J. Schultz
    • William J. Schultz
    • B27N3/20D21J1/00D21J1/04D21J1/18
    • D21J1/04B27N3/20D21J1/00B29K2311/14
    • Panels of composite wood material are formed in a wet process which includes depositing a layer of wet composite wood material in a mat on a press wire screen mesh and moving the screen mesh to carry the mat into a pressing position between a pair of spaced apart pressure plates having generally matching, contoured facing surfaces for shaping the outer face and a smoothly contoured back face of the panel. The back face of the panel is not flat and generally follows or matches the shape or contour of the outer face so that regions of high fiber stress and dense, brittle areas of high fiber compression are generally eliminated. The resulting finished panels having excellent machining qualities, more uniform surface coating absorption characteristics, more uniform thickness and less rapid moisture absorption properties, along with a lower tendency to check, crack or split.
    • 复合木材材料的面板是以湿法形成的,其中包括将湿复合木材材料层沉积在压丝网筛上的垫中,并移动筛网以将垫运送到一对隔开的压力 板具有大体上匹配的,轮廓的面对表面,用于成形外表面和平滑轮廓的面板。 面板的背面不平坦,通常与外表面的形状或轮廓相符或匹配,因此高纤维应力的区域和高纤维压缩的致密,脆性区域通常被消除。 所得到的成品面板具有优异的加工性能,更均匀的表面涂层吸收特性,更均匀的厚度和更少的快速吸湿性能,以及更低的检查,裂缝或分裂倾向。
    • 37. 发明授权
    • Compositions for making ene-thiol elastomers
    • 制备烯 - 硫醇弹性体的组合物
    • US06605691B1
    • 2003-08-12
    • US10252273
    • 2002-09-23
    • Kathleen B. GrossWilliam J. Schultz
    • Kathleen B. GrossWilliam J. Schultz
    • C08G7504
    • C08G75/045C08G75/12H05K3/285
    • In one aspect, the invention provides ene-thiol elastomers comprising the reaction product of a polythiol free of hydrophilic groups and having at least two thiol groups and an aromatic, heterocyclic, aliphatic, or cycloaliphatic polyene having at least two reactive unsaturated carbon to carbon bonds. In another aspect, the invention provides ene-thiol elastomer comprising the reaction product of (a) a thiol terminated oligomer comprising the reaction product of a polythiol having two thiol groups and a first polyene or mixture of polyenes having two reactive unsaturated carbon to carbon bonds; and (b) a second polyene or a mixture of polyenes having at least 5 percent functional equivalents of unsaturated carbon to carbon bonds from polyenes having at least three unsaturated carbon to carbon bonds. The ene-thiol elastomers of the invention have a weight increase of not more than 4 weight percent in 15 days at a temperature of 22 ° C. when immersed in a solution of 96 parts by weight water and 4 parts by weight n-butanol and/or a water vapor transmission rate of less than 50 g-mm/m2-day at 40 ° C. according to ASTM D814.
    • 一方面,本发明提供了包含不含亲水基团且具有至少两个巯基的多硫醇和具有至少两个反应性不饱和碳 - 碳键的芳族,杂环,脂族或脂环族多烯的反应产物的烯 - 硫醇弹性体 。 另一方面,本发明提供了包含(a)包含具有两个硫醇基的多硫醇的反应产物和具有两个反应性不饱和碳与碳键的第一多烯或多烯混合物的硫醇封端低聚物的反应产物的烯 - 硫醇弹性体 ; 和(b)具有至少3个不饱和碳 - 碳键的多烯具有至少5%的不饱和碳与碳键的功能当量的至少5%的多烯或多烯的混合物。 本发明的烯硫醇弹性体在浸渍在96重量份水和4重量份正丁醇的溶液中时,在22℃的温度下15天内的重量增加不超过4重量%, /或根据ASTM D814在40℃下小于50g-mm / m 2·天的水蒸汽透过率。