    • 30. 发明授权
    • Method for producing seamless steel pipe
    • 无缝钢管生产方法
    • US08361256B2
    • 2013-01-29
    • US12010433
    • 2008-01-24
    • Yuji AraiKeiichi Nakamura
    • Yuji AraiKeiichi Nakamura
    • C21D9/08C22C38/00C22C38/22
    • C22C38/02C21D8/105C21D9/08C22C38/04C22C38/22C22C38/24C22C38/28C22C38/32
    • A seamless steel pipe produced by heating a steel billet, which has a chemical composition C: 0.15 to 0.20%, Si: not less than 0.01% to less than 0.15%, Mn: 0.05 to 1.0%, Cr: 0.05 to 1.5%, Mo: 0.05 to 1.0%, Al≦0.10%, V: 0.01 to 0.2%, Ti: 0.002 to 0.03%, B: 0.0003 to 0.005% and N: 0.002 to 0.01%, further optionally one or more of Ca, Mg and REM in a specific amount, under the provision that the conditions “C+(Mn/6)+(Cr/5)+(Mo/3)≧0.43” and “Ti×N
    • 通过将化学组成C:0.15〜0.20%,Si:0.01〜0.15%,Mn:0.05〜1.0%,Cr:0.05〜1.5%的钢坯加热而制造的无缝钢管, Mo:0.05〜1.0%,Al≤1.0%,0.10%,V:0.01〜0.2%,Ti:0.002〜0.03%,B:0.0003〜0.005%,N:0.002〜0.01% REM满足条件C +(Mn / 6)+(Cr / 5)+(Mo / 3)≥0.43,Ti×N <0.0002〜0.0006×Si的条件,其余为Fe 和杂质,其中杂质中的P <0.01; 0.025%,S&NlE; 0.010%和Nb <0.005%,至1000〜1250℃的温度,随后在最终轧制温度900〜1050℃下进行制管轧制, 然后从不低于Ar3相变点的温度直接淬火所得到的钢管,然后在600℃至Ac1相变点的温度范围内回火,或者在所述制管轧制之后代替上述 在从Ac3相变点到1000℃的温度范围内串联加热所得到的钢管,然后从不低于Ar 3相变点的温度淬火,然后在600℃的温度范围内回火。 到Ac1转化点,具有高强度和优异的韧性,同时具有高产率,并且具有优异的耐SSC性。