    • PCT No. PCT/SE93/00136 Sec. 371 Date Aug. 19, 1994 Sec. 102(e) Date Aug. 19, 1994 PCT Filed Feb. 19, 1993 PCT Pub. No. WO93/16836 PCT Pub. Date Sep. 2, 1993.A method of cladding an outer tube (1) with an inner tube (2), wherein the inner tube is made of a corrosion-resistant material, for instance. The inventive is characterized by placing a number of explosive charges (3) in mutually spaced arrangement in the inner tube (2), in contact with or essentially in contact with the inner surface of the inner tube; filling the inner tube with a pressure-transmitting medium (4), preferably water; and detonating all explosive charges (3) simultaneously, so as to obtain a local metallurgical bond (6) at the regions of the explosive charges and so as to cause the inner tube (2) to expand into abutment with the outer tube (1).
    • 24. 发明专利
    • A METHOD OF EXPLOSION WELDING ALLOY ALUMINIUM
    • GB2210307B
    • 1991-09-18
    • GB8822218
    • 1988-09-21
    • EXPLOWELD AB
    • PERSSON INGEMAR
    • B23K20/08B23K20/227
    • A method of explosion welding magnesium-alloyed aluminium to high strength material. The invention is characterized in that the magnesium-alloyed aluminium material comprises base material (4) and that the base material is clad or coated with a thin cladding plate (3) consisting of the afore mentioned high strength material, in that an explosive charge (1) is caused to accelerate a drive plate (2) made of a high density material, preferably steel, which in turn is arranged to accelerate the cladding material (3) towards the base material (4), where the amplitude of the pressure generated between the cladding material and the base material is caused to take a value which is so low that the temperature in the whole of the joint surface, or substantially the whole of the joint surface, is below the boiling point of the alloying substances of the aluminium material, while bringing, at the same time, the amplitude or duration of this pressure to such a high level as to produce an impulse which is sufficient to cause the materials to weld to one another, and in that the free surface of the high-strength cladding material (3) is explosion welded, in a later stage, to a base material (6) consisting of steel or some other high strength metal.