会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 21. 发明专利
    • Electrolyte
    • 电解液
    • JP2013110006A
    • 2013-06-06
    • JP2011254939
    • 2011-11-22
    • Toyota Central R&D Labs Inc株式会社豊田中央研究所
    • FUJITA SATORUHASEGAWA NAOKIKAWAKADO MASAYA
    • H01B1/06C01B33/12H01M8/02H01M8/10
    • Y02E60/521
    • PROBLEM TO BE SOLVED: To provide an electrolyte having a high EW (or a low IEC), and exhibiting a high proton conductivity even in non-humidified conditions.SOLUTION: The electrolyte includes a silica layer formed by condensation polymerization of a hydrophilic group consisting of a silanol group or a precursor thereof, and an organic sulfonate group modifying the internal surface of the silica layer and not having pores derived from the removal of a surfactant internally. The electrolyte is obtained by adding an SiOsource having a hydrophilic group, as required, into a solution containing amphipathic molecules including a silanol group or a hydrophilic group consisting of a precursor thereof and a hydrophobic group consisting of a precursor of an organic sulfonate group, self-assembling the amphipathic molecules in the solution, and condensing and polymerizing the hydrophilic group.
    • 要解决的问题:提供具有高EW(或低IEC)的电解质,即使在非加湿条件下也表现出高的质子传导性。 解决方案:电解质包括通过由硅烷醇基或其前体组成的亲水基团的缩聚形成的二氧化硅层和改性二氧化硅层的内表面并且不具有来自除去的孔的有机磺酸盐基团 的表面活性剂。 电解质是通过将根据需要将具有亲水基团的SiO 2原料添加到含有两亲性分子的溶液中而获得的,所述两亲分子包括硅烷醇基或由其前体组成的亲水基团, 由有机磺酸盐基团的前体组成的疏水基团,在溶液中自组装两亲性分子,并使亲水基团缩合和聚合。 版权所有(C)2013,JPO&INPIT
    • 24. 发明专利
    • Material coated with metal single atomic layer and manufacturing method therefor
    • 材料涂覆金属单原子层及其制造方法
    • JP2012046775A
    • 2012-03-08
    • JP2010187632
    • 2010-08-24
    • Toyota Central R&D Labs Inc株式会社豊田中央研究所
    • UETAKA YUJITAKESHITA TOMOHIROJINNAI AKINORIHATANAKA TATSUYAKAWAKADO MASAYAMORIMOTO TOMO
    • C23C14/14
    • PROBLEM TO BE SOLVED: To provide a material coated with a metal single atomic layer where the surface of the substrate is coated with a metal single atomic layer, and manufacturing method therefor.SOLUTION: The method includes: a sealing step of sealing a first substrate and a coating metal which satisfy a predetermined relationship among affinity, a melting point and an evaporation temperature, in a sealed container so as to form the metal single atomic layer; and a coating step of coating a surface of the first substrate with the metal single atomic layer comprising the coating metal after the sealed container is heated at a maximum value Tor higher of the evaporation temperature in a vacuum of each coating metal, and at a lower temperature or below between a minimum value of the temperature at which each first substrate and coating metal react and a heat resistant temperature of the sealed container, and the sealed container is then cooled.
    • 要解决的问题:提供涂覆有金属单原子层的材料,其中基底的表面被金属单原子层涂覆,及其制造方法。 解决方案:该方法包括:在密封容器中密封在亲和力,熔点和蒸发温度之间满足预定关系的第一基底和涂层金属的密封步骤,以形成金属单原子层 ; 以及在密封容器被加热到​​最大值T Mb 以上之后,将包含涂层金属的金属单原子层涂覆在第一基板的表面上的涂布步骤 在每个涂覆金属的真空中的蒸发温度以及在每个第一基底和涂覆金属反应的温度的最小值与密封容器的耐热温度之间的较低温度或更低温度下,然后将密封容器冷却 。 版权所有(C)2012,JPO&INPIT
    • 28. 发明专利
    • Strong acid crosslinking type compound electrolyte
    • 强酸交联型复合电解质
    • JP2009259793A
    • 2009-11-05
    • JP2009062881
    • 2009-03-16
    • Toyota Central R&D Labs Inc株式会社豊田中央研究所
    • TSUSAKA KYOKOKAMIYA ATSUSHIHASEGAWA NAOKIKAWAKADO MASAYA
    • H01B1/06C08F2/44C08F283/00C08G75/30H01M8/02
    • Y02E60/50
    • PROBLEM TO BE SOLVED: To provide a strong acid crosslinking type compound electrolyte capable of providing compatibility between strength and electric conductivity. SOLUTION: The strong acid crosslinking type compound electrolyte includes a high polymer electrolyte containing imide crosslinking type electrolyte provided by a reaction of one or more types of first monomers having two or more reactive functional groups A, B, and one or more types of second monomers having three or more of the reactive functional groups A, B, and a different type of polymer combined with the imide crosslinking type electrolyte. At least one reactive functional group A, and at least one reactive functional group B are included in either one of the first monomer or the second monomer. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供能够提供强度和电导率之间的相容性的强酸交联型复合电解质。 解决方案:强酸交联型复合电解质包括通过一种或多种具有两个或更多个反应性官能团A,B和一种或多种类型的第一单体的反应提供的含有酰亚胺交联型电解质的高分子电解质 的具有三个或更多个反应性官能团A,B的第二单体和与酰亚胺交联型电解质组合的不同类型的聚合物。 至少一个反应性官能团A和至少一个反应性官能团B包括在第一单体或第二单体中的任一个中。 版权所有(C)2010,JPO&INPIT
    • 29. 发明专利
    • Composite electrolyte, and its manufacturing method
    • 复合电解质及其制造方法
    • JP2008243511A
    • 2008-10-09
    • JP2007080720
    • 2007-03-27
    • Toyota Central R&D Labs Inc株式会社豊田中央研究所
    • HOSOKAWA YOICHITSUSAKA KYOKOHASEGAWA NAOKIKAWAKADO MASAYA
    • H01B13/00C08J9/36H01B1/06H01M8/02H01M8/10
    • Y02P70/56
    • PROBLEM TO BE SOLVED: To provide a composite electrolyte suppressing elution and swell of the electrolyte, high in electric conductivity, and excelling in chemical durability, and also to provide its manufacturing method. SOLUTION: This composite electrolyte manufacturing method comprises: a modification process of introducing a reactive functional group A comprising a sulfonamide group or its derivative, or a sulfonyl halide group or its derivative into a surface of a hydrocarbon-based porous base material; and a compounding process of filling an electrolyte monomer and/or an electrolyte polymer having a reactive functional group B producing a sulfonimide group by reacting with the reactive functional group A in the hydrocarbon-based porous base material to react the reactive functional group A with the reactive functional group B. This composite electrolyte is provided by such a method. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供抑制电解质的洗脱和膨胀的复合电解质,高导电性和优异的化学耐久性,并且还提供其制造方法。 解决方案:该复合电解质制造方法包括:将包含磺酰胺基团或其衍生物或磺酰卤基团或其衍生物的反应性官能团A引入烃类多孔基材的表面的改性方法; 以及填充电解质单体和/或具有反应性官能团B的电解质聚合物的复合方法,通过与烃类多孔基材中的反应性官能团A反应,使反应性官能团A与 反应性官能团B.这种复合电解质是通过这种方法提供的。 版权所有(C)2009,JPO&INPIT