    • 15. 发明授权
    • Method for producing modified conjugated diene polymer and rubber composition
    • 改性共轭二烯聚合物和橡胶组合物的制备方法
    • US07202306B2
    • 2007-04-10
    • US10849786
    • 2004-05-21
    • Ryouji TanakaTakuo SoneToshihiro Tadaki
    • Ryouji TanakaTakuo SoneToshihiro Tadaki
    • C08F36/06C08C19/25
    • C08L19/006C08C19/25C08C19/34C08C19/42C08L21/00C08L2666/08
    • Disclosed are a method for producing a modified conjugated diene polymer improved in quality stability, more enhanced in low heat buildup and reinforcing ability when used in a rubber composition, excellent in wear resistance, mechanical characteristics and processability, and improved in cold flow; and a rubber composition using the same. The method includes a step of modifying an active end of an active end-containing conjugated diene polymer having a cis-1,4-bond content of 75% or more with an alkoxysilane compound containing at least one functional group selected from the group consisting of (a) an epoxy group, (b) an isocyanate group and (c) a carboxyl group, and a step of adding a condensation accelerator to conduct condensation reaction of the alkoxysilane compound (residue) in an aqueous solution having a pH of 9 to 14 and a temperature of 85 to 180° C.
    • 公开了一种制备改性共轭二烯聚合物的方法,该改性共轭二烯聚合物在橡胶组合物中使用时质量稳定性提高,低发热性和增强能力提高,耐磨性,机械特性和加工性优异,冷流改善; 和使用其的橡胶组合物。 该方法包括使含有至少一个选自以下的官能团的烷氧基硅烷化合物改性具有75%以上的顺式-1,4-键含量的含活性端的共轭二烯聚合物的活性末端的步骤: (a)环氧基,(b)异氰酸酯基和(c)羧基,以及加入缩合促进剂以使烷氧基硅烷化合物(残基)在pH为9的水溶液中进行缩合反应的步骤, 14℃,温度为85〜180℃。