    • 18. 发明授权
    • Method of applying phosphor coatings
    • 施加荧光体涂层的方法
    • US08282986B2
    • 2012-10-09
    • US11750023
    • 2007-05-17
    • Richard S. SpeerMadis Raukas
    • Richard S. SpeerMadis Raukas
    • B05D5/06B05D3/02
    • C09K11/0883C09K11/02C09K11/7706C09K11/7734
    • A method of applying a phosphor coating is described. The method comprises forming a suspension of a phosphor and a polymer binder dissolved in a solvent, the phosphor comprising at least one of a nitridosilicate or an oxonitridosilicate phosphor, the polymer binder being capable of decomposing thermally; applying the suspension to a substrate to form a coating; drying the coating; and baking the coating in an inert atmosphere to thermally decompose the polymer binder to form the phosphor coating, preferably at a temperature less than about 400° C. in a nitrogen atmosphere. A preferred polymer binder is polyisobutyl methacrylate
    • 描述了施加荧光体涂层的方法。 所述方法包括形成溶解在溶剂中的磷光体和聚合物粘合剂的悬浮液,所述荧光体包括氮化硅酸盐或氧代烟草硅酸盐荧光体中的至少一种,所述聚合物粘合剂能够热分解; 将悬浮液施加到基底以形成涂层; 干燥涂层; 并在惰性气氛中烘烤该涂层以热分解聚合物粘合剂以形成荧光体涂层,优选在氮气气氛中在低于约400℃的温度下进行。 优选的聚合物粘合剂是甲基丙烯酸异丁酯
    • 19. 发明授权
    • Highly loaded fluorescent lamp
    • 高负载荧光灯
    • US06777867B2
    • 2004-08-17
    • US10344103
    • 2003-02-10
    • Kailiah MishraMadis RaukasCathy M Shaw Trumble
    • Kailiah MishraMadis RaukasCathy M Shaw Trumble
    • H01J162
    • C09K11/7734C09K11/7777C09K11/7787H01J61/44H01J61/48H01J65/00
    • A highly loaded fluorescent lamp (10) (FIG. 1) comprises a hollow, translucent glass body (12) containing a medium capable of generating at least several wavelengths of UV radiation. A plurality of phosphors is disposed on the inside surface of the glass body (12), the plurality of phosphors visible radiation upon exposure to the UV radiation. At least one of the plurality of phosphors is subject to degradation upon lone-term exposure to one of the at least one of several wavelengths of UV radiation. The at least one of the plurality of phosphors subject to degradation is installed (FIG. 12) adjacent the inside surface (14) of the glass body (12) to form a first layer (16); and the remainder of the plurality of phosphors is disposed on the first layer to form a second layer (18), the second layer not being subject to long-term degradation upon exposure to the UV radiation.
    • 高负载荧光灯(10)(图1)包括中空的半透明玻璃体(12),其包含能够产生至少几个紫外辐射波长的介质。 多个磷光体设置在玻璃体(12)的内表面上,多个磷光体在暴露于紫外线辐射时可见光。 多个荧光体中的至少一个在单次暴露于若干波长的紫外线辐射中的至少一个中的一个时遭受降解。 与玻璃体(12)的内表面(14)相邻的多个荧光体中的至少一个被劣化地安装(图12)以形成第一层(16); 并且所述多个磷光体的其余部分设置在所述第一层上以形成第二层(18),所述第二层在暴露于所述UV辐射时不会长期劣化。