    • 12. 发明专利
    • METHOD FOR HOT ROLLING PARTIALLY JOINED PART OF STEEL STRIP
    • JPH0663605A
    • 1994-03-08
    • JP21889992
    • 1992-08-18
    • KAWASAKI STEEL CO
    • KANARI SHOHEIISOBE KUNIOYARITA YUKIOYORIFUJI AKIRA
    • B21B1/26B21B15/00B21B45/02
    • PURPOSE:To improve joining strength in a joined part by rolling a steel strip after temporally stopping the application of a lubricant and starting the application of a friction increasing agent when the partially joined part of the steel strip reaches a specified position on the inlet side of a rolling mill. CONSTITUTION:Just before a material to be rolled is bitten with rolls, i.e., at the time of T1 before, the friction increasing agent is applied, the application of the friction increasing agent is stopped at the time of T2 after the material to be rolled is bitten with the rolls and immediately a lubricant is applied. After that, rolling is continued and, when the scheduled biting time of the partially joined part is detected with a joined part detector, the application of the lubricant is stopped at the time of T3 before when is preceding to the time of the application of the friction increasing agent to the partially joined part and the application of the friction increasing agent is started after an elapse of the time of T3. Next, at the time of T2 after the end of the joined part passes through, the application of the friction increasing agent is stopped and immediately the application of the lubricant is restarted. Then, the time of (T1+T2) is measured from the time when the joined part reaches the position of at least the circumferential length of the rolling roll from a roll biting point.