    • CREPING ADHESIVES AND METHODS FOR MAKING AND USING SAME
    • KREPPHAFTSTOFFE UND VERFAHREN ZUR HERSTELLUNG UND VERWENDUNG DAVON
    • EP3066261A4
    • 2017-07-19
    • EP14859971
    • 2014-11-07
    • GEORGIA-PACIFIC CHEMICALS LLC
    • RINGOLD CLAY ETOWNSEND DAVID FHAGIOPOL CORNELFAVORS KARLA DWRIGHT THOMAS L
    • D21H17/55C08G73/02C09J179/02D21H17/46
    • D21H21/146C08G73/0286C08L79/02C09J179/02C09J2479/02D21H17/07D21H17/15D21H17/56D21H17/72
    • Creping adhesives and methods for making and using same are provided. The creping adhesive can include a first thermosetting polyamidoamine-epihalohydrin resin that includes a reaction product of a first epihalohydrin and a first polyamidoamine containing one or more secondary amine groups, a first thermoplastic polyamidoamine-epihalohydrin resin that includes a reaction product of a second epihalohydrin and a second polyamidoamine containing one or more secondary amine groups, and one or more re-wetting agents. The first thermosetting polyamidoamine-epihalohydrin resin can have a weight average molecular weight of about 800,000 to about 1,200,000 and a molar ratio of the first epihalohydrin to the secondary amine groups of about 0.002:1 to about 0.1:1. The first thermoplastic polyamidoamine-epihalohydrin resin can have a weight average molecular weight of about 40,000 to about 200,000 and a molar ratio of the second epihalohydrin to the secondary amine groups of about 0.001:1 to about 0.1:1.
    • 提供起皱粘合剂及其制造和使用方法。 起皱粘合剂可以包括第一热固性聚酰胺胺 - 表卤代醇树脂,其包括第一表卤代醇和含有一个或多个仲胺基团的第一聚酰胺胺的反应产物,第一热塑性聚酰胺胺 - 表卤代醇树脂,其包括第二表卤代醇和 含有一个或多个仲胺基团的第二聚酰胺胺和一种或多种再润湿剂。 第一热固性聚酰胺胺 - 表卤代醇树脂可具有约800,000至约1,200,000的重均分子量和约0.002:1至约0.1:1的第一表卤代醇与仲胺基团的摩尔比。 第一热塑性聚酰胺胺 - 表卤代醇树脂可具有约40,000至约200,000的重均分子量和约0.001:1至约0.1:1的第二表卤代醇与仲胺基团的摩尔比。