    • 92. 发明授权
    • Hard facing nickel-base alloy
    • 硬面镍基合金
    • US4404049A
    • 1983-09-13
    • US189843
    • 1980-10-24
    • Kanichi TanakaKensuke Hidaka
    • Kanichi TanakaKensuke Hidaka
    • B23K35/30C22C19/05
    • C22C19/05B23K35/304
    • Hard facing nickel-base alloys comprising 0.05 to 1.5% by weight of boron, 3 to 7% by weight of silicon, 7.5 to 35% by weight of chromium, 0.05 to 1.5% by weight of carbon, and if necessary, less than 30% by weight of iron and/or less than 5% by weight of tungsten, the balance being nickel, with the weight ratio of silicon to boron being equivalent to or exceeding 3.3. The alloys have a high degree of toughness, ductility, wear resistance and corrosion resistance, and no cracks occur in the hard facing layer. Addition of 0.1 to 3% by weight of the tin and/or 0.1 to 3% by weight of tantalum remarkably increases the corrosion resistance. The alloys can be used as a hard facing material to be applied to parts of various instruments, machines and plants.
    • PCT No.PCT / JP79 / 00026 Sec。 371日期1979年10月24日 102(e)日期1979年10月24日PCT提交1979年2月5日PCT公布。 出版物WO79 / 00772 日期为1979年10月4日。面对镍基合金,其包含0.05至1.5重量%的硼,3至7重量%的硅,7.5至35重量%的铬,0.05至1.5重量%的碳, 如果需要,小于30重量%的铁和/或小于5重量%的钨,余量为镍,硅与硼的重量比等于或超过3.3。 合金具有高韧性,延展性,耐磨性和耐腐蚀性,并且在硬面层中不发生裂纹。 添加0.1〜3重量%的锡和/或0.1〜3重量%的钽显着提高耐腐蚀性。 该合金可以用作硬面材料,以应用于各种仪器,机器和设备的部件。