    • 1. 发明授权
    • Production of ferrovanadium alloys
    • 生产富镁合金
    • US3637370A
    • 1972-01-25
    • US3637370D
    • 1968-06-10
    • FOOTE MINERAL CO
    • BUKER DONALD O
    • C22C33/00C22C1/00C22B55/00
    • C22C33/003
    • A method of producing a low-carbon low-oxygen ferrovanadium alloy by carbon reduction in which an agglomerated mixture of comminuted vanadium oxide, preferably a pentoxide, an iron-source material, and a carbon-source material are heated in vacuum to a temperature of 2,400*-2,800* F. The temperature is maintained until evolution of gas substantially ceases and the product fuses. Additional agglomerate can be charged into the vacuum environment without breaking the vacuum, and molten alloy continuously collected to provide a substantially continuous process.
    • 一种通过碳还原生产低碳低氧钒铁合金的方法,其中粉碎的氧化钒,优选五氧化二钒,铁源材料和碳源材料的凝聚混合物在真空中加热至 温度保持恒定,直至气体放出基本停止,产品保温。 可以将附加的附聚物装入真空环境中而不破坏真空,并且连续收集熔融合金以提供基本连续的工艺。
    • 10. 发明授权
    • Vanadium recovery process
    • VANADIUM RECOVERY PROCESS
    • US3656936A
    • 1972-04-18
    • US3656936D
    • 1970-10-14
    • OIL SHALE CORP
    • HAAS FRANK C
    • C22B34/22C22B55/00
    • C22B34/22
    • A process is provided for recovering vanadium values from highly alkaline, calcium-rich calcines, which are usually the roasted product of low-grade vanadium-bearing calcitic ores. The process involves slurrying the calcine in water and carbonating the slurry to a pH of 5.0 to 9.0 to extract the soluble vanadium species from the slurry. A basic anion exchange resin is added to the carbonated slurry thereby increasing the vanadium recovery by shifting the extraction equilibrium.
    • 提供了一种从高碱性,富钙的煅烧回收钒值的方法,通常是低品位含钒方解石矿石的焙烤产品。 该方法包括将煅烧物浆化成水,并将浆料碳酸化至5.0至9.0的pH以从浆料中提取可溶性钒物质。 向碳酸化浆料中加入碱性阴离子交换树脂,从而通过转移萃取平衡来提高钒回收率。