    • 2. 发明授权
    • Two-component coating compositions
    • 双组分涂料组合物
    • US09458351B2
    • 2016-10-04
    • US14115077
    • 2012-05-03
    • Wiebke BeckerKatharina DregerCarmen Flosbach
    • Wiebke BeckerKatharina DregerCarmen Flosbach
    • C09D163/00C08G18/62C08G18/79C09D175/04C08G18/22C08G18/24
    • C09D163/00C08G18/22C08G18/246C08G18/6229C08G18/6254C08G18/6258C08G18/792C09D175/04
    • Two-component coating compositions include: A) a cross-linkable binder compound having at least one functional group reactive towards isocyanate groups, B) a cross-linking agent having at least one free isocyanate group and C) a catalyst component comprising C1) a catalyst for the for the curing reaction between the functional groups of component A) and the isocyanate groups of component B), the catalyst C1) being an organo-metal compound, and C2) an oligomeric or polymeric binder compound having a glass transition temperature Tg of ≧about 20° C., measured by DSC (differential scanning calorimetry) at a heating rate of 10 K/min. The glass transition temperature Tg of the binder compound C2) is above the temperature at which the two-component coating composition is applied, preferably about 10° C. above the temperature at which the two-component coating composition is applied.
    • 双组分涂料组合物包括:A)具有至少一个对异氰酸酯基团具有反应性的官能团的可交联粘合剂化合物,B)具有至少一个游离异氰酸酯基团的交联剂,和C)包含C1) 用于组分A)的官能团与组分B)的异氰酸酯基团之间的固化反应的催化剂,催化剂C1)是有机金属化合物,和C2)具有玻璃化转变温度Tg的低聚或聚合的粘合剂化合物 通过DSC(差示扫描量热法)以10K / min的加热速率测量。 粘合剂化合物C2)的玻璃化转变温度Tg高于施加双组分涂料组合物的温度,优选在高于施加双组分涂料组合物的温度下约10℃。
    • 4. 发明授权
    • Coating compositions and process for the production of multilayer coatings
    • 涂料组合物和生产多层涂料的方法
    • US07960468B2
    • 2011-06-14
    • US10953311
    • 2004-09-29
    • Wiebke BeckerVolker DuecoffreCarmen FlosbachBirgit Kleuser
    • Wiebke BeckerVolker DuecoffreCarmen FlosbachBirgit Kleuser
    • C08L31/00C08L33/00C08L51/00C08L67/00C08L75/00
    • C09D175/04C08G18/4063C08G2270/00
    • An aqueous coating composition, comprisingA) at least one water-dilutable hydroxy-functional binder andB) at least one polyisocyanate crosslinking agent with free isocyanate groups,wherein component A) comprises A1) 40-95 wt. % of at least one water-dilutable hydroxy-functional (meth)acrylic copolymer with a hydroxyl value of 60-250 mg of KOH/g and an acid value of 5-50 mg of KOH/g, which is obtained by free-radical copolymerization performed in a non-aqueous phase, wherein the ratio of primary hydroxyl groups to secondary hydroxyl groups in the (meth)acrylate copolymer A1) is 1:0.1 to 1:1.2 and at least 80% of the secondary hydroxyl groups result from reaction products of a monoepoxy ester and an unsaturated acid-functional monomer, and A2) 5-60 wt. % of at least one water-dilutable polyester oligomer, wherein the total of the weight percentages of component A1) and A2) add up to 100 wt. % and wherein the free-radical polymerization for the production of component A1) is performed at least in part in the presence of component A2) and/or wherein component A2) is added during polymerization or after completion of polymerization.
    • 一种水性涂料组合物,其包含A)至少一种水可稀释的羟基官能粘合剂和B)至少一种具有游离异氰酸酯基团的多异氰酸酯交联剂,其中组分A)包括A1)40-95wt。 %的羟基值为60-250mg KOH / g和酸值为5-50mg KOH / g的水可稀释的羟基官能(甲基)丙烯酸共聚物的%,它是通过自由基 在非水相中进行共聚,其中(甲基)丙烯酸酯共聚物A1)中伯羟基与仲羟基的比例为1:0.1至1:1.2,并且至少80%的仲羟基由反应产生 单环酯和不饱和酸官能单体的产物,和A2)5-60wt。 %的至少一种水可稀释的聚酯低聚物,其中组分A1)和A2)的总重量百分比加到100wt。 %,并且其中用于制备组分A1)的自由基聚合至少部分地在组分A2)和/或其中组分A2)的存在下进行,或者聚合期间或聚合完成后加入组分A2)。
    • 7. 发明申请
    • Coating compositions and process for the production of multilayer coatings
    • 涂料组合物和生产多层涂料的方法
    • US20060069202A1
    • 2006-03-30
    • US10953311
    • 2004-09-29
    • Wiebke BeckerVolker DuecoffreCarmen FlosbachBirgit Kleuser
    • Wiebke BeckerVolker DuecoffreCarmen FlosbachBirgit Kleuser
    • C08L75/00
    • C09D175/04C08G18/4063C08G2270/00
    • An aqueous coating composition, comprising A) at least one water-dilutable hydroxy-functional binder and B) at least one polyisocyanate crosslinking agent with free isocyanate groups, wherein component A) comprises A1) 40-95 wt. % of at least one water-dilutable hydroxy-functional (meth)acrylic copolymer with a hydroxyl value of 60-250 mg of KOH/g and an acid value of 5-50 mg of KOH/g, which is obtained by free-radical copolymerization performed in a non-aqueous phase, wherein the ratio of primary hydroxyl groups to secondary hydroxyl groups in the (meth)acrylate copolymer A1) is 1:0.1 to 1:1.2 and at least 80% of the secondary hydroxyl groups result from reaction products of a monoepoxy ester and an unsaturated acid-functional monomer, and A2) 5-60 wt. % of at least one water-dilutable polyester oligomer, wherein the total of the weight percentages of component A1) and A2) add up to 100 wt. % and wherein the free-radical polymerization for the production of component A1) is performed at least in part in the presence of component A2) and/or wherein component A2) is added during polymerization or after completion of polymerization.
    • 一种水性涂料组合物,其包含A)至少一种水可稀释的羟基官能粘合剂和B)至少一种具有游离异氰酸酯基团的多异氰酸酯交联剂,其中组分A)包括A1)40-95wt。 %的羟基值为60-250mg KOH / g和酸值为5-50mg KOH / g的水可稀释的羟基官能(甲基)丙烯酸共聚物的%,它是通过自由基 在非水相中进行共聚,其中(甲基)丙烯酸酯共聚物A1)中伯羟基与仲羟基的比例为1:0.1至1:1.2,并且至少80%的仲羟基由反应产生 单环酯和不饱和酸官能单体的产物,和A2)5-60wt。 %的至少一种水可稀释的聚酯低聚物,其中组分A1)和A2)的总重量百分比加到100wt。 %,并且其中用于生产组分A1)的自由基聚合至少部分地在组分A2)和/或其中组分A2)的存在下进行,或者聚合期间或聚合完成后加入。
    • 9. 发明申请
    • PROCESS FOR PAINTING SUBSTRATES
    • 绘制基材的方法
    • US20100279016A1
    • 2010-11-04
    • US12738339
    • 2008-10-01
    • Carmen FlosbachAndrew HearleyWiebke BeckerJuergen Stropp
    • Carmen FlosbachAndrew HearleyWiebke BeckerJuergen Stropp
    • B05D3/02
    • C08G18/282C09D175/04
    • The invention relates to a process for painting substrates comprising the following steps: 1. applying a coating composition to an optionally pre-coated substrate and 2. hardening the applied coating composition, wherein the coating composition comprises: A) at least one binder having functional groups containing active hydrogen, B) at least one polyisocyanate cross-linking agent having free isocyanate groups and C) at least one urethane compound having at least two —O—CO—NH— groups, wherein the urethane compound is substantially free from functional groups which are capable of entering into a cross-linking reaction with components A) and/or B) and wherein the hardening is carried out under conditions such that the component C) does not contribute to the cross-linking of the applied coating composition by chemical reaction.
    • 本发明涉及一种用于涂布基材的方法,包括以下步骤:1.将涂料组合物施用到任选预涂的基材上,和2.硬化涂覆的涂料组合物,其中涂料组合物包含:A)至少一种具有官能 含有活性氢的基团,B)至少一种具有游离异氰酸酯基团的多异氰酸酯交联剂,和C)至少一种具有至少两个-O-CO-NH-基团的氨基甲酸酯化合物,其中氨基甲酸酯化合物基本上不含官能团 其能够与组分A)和/或B)进行交联反应,并且其中所述硬化在使得组分C)不有助于通过化学品施用的涂料组合物的交联的条件下进行 反应。