    • 2. 发明申请
    • USE OF A CATALYST COMPRISING A PHOSPHORUS MODIFIED ZEOLITE IN AN ALCOHOL DEHYDRATION PROCESS
    • 在酒精脱水过程中使用包含磷酸改性沸石的催化剂
    • WO2013017496A1
    • 2013-02-07
    • PCT/EP2012/064579
    • 2012-07-25
    • TOTAL RESEARCH & TECHNOLOGY FELUYIFP Energies nouvellesNESTERENKO, NikolaiMINOUX, DelphineADAM, CindyDATH, Jean-PierreLOPEZ, JosephEUZEN, Patrick
    • NESTERENKO, NikolaiMINOUX, DelphineADAM, CindyDATH, Jean-PierreLOPEZ, JosephEUZEN, Patrick
    • B01J29/40B01J29/85B01J37/10B01J37/28C07C1/20
    • C07C1/24B01J29/40B01J29/85B01J37/10B01J37/28C07C2527/14C07C2529/06C07C2529/40Y02P20/52Y02P30/42C07C11/04
    • The present invention relates, in a first embodiment, to the use of a catalyst to convert at least an alcohol into light olefins in a dehydration process to make an olefin having the same number of carbon atoms as the alcohol wherein said catalyst comprises a phosphorus modified zeolite and is made by a method comprising the following steps in this order, a) providing a zeolite comprising at least one ten members ring in the structure, optionally steaming said zeolite, b) mixing said zeolite of step a) with at least a component selected among one or more binders and shaping additives, then shaping said mixture, c) optionally making a ion-exchange, d) optionally steaming the shaped catalyst, optionally before step c), at least among said steaming of step d) and the steaming of step a) one is mandatory, e) introducing phosphorus on the catalyst to introduce at least 0.1 wt% of phosphorus, said introduction being made by dry impregnation or chemical vapor deposition, f) optionally introducing a metal, optionally simultaneously with step e), g) optionally washing the catalyst, h) optionally calcinating the catalyst, i) steaming the catalyst, also referred to as the equilibration step. In a second embodiment phosphorus can be introduced by any means and at step i) the steaming severity (X) is at least about 2. In said second embodiment the catalyst is advantageously steamed at a temperature above 625°C, preferably in the range 700 to 800°C. The metal of step f) is advantageously Calcium.
    • 在第一个实施方案中,本发明涉及在脱水方法中使用催化剂将至少一种醇转化为轻质烯烃,以制备具有与醇相同数目的碳原子的烯烃,其中所述催化剂包含磷改性 沸石,并且通过包括以下步骤的方法制备:a)提供在该结构中包含至少一个十元环的沸石,任选地蒸汽所述沸石,b)将步骤a)的所述沸石与至少一种组分 选自一种或多种粘合剂和成型添加剂,然后成型所述混合物,c)任选地进行离子交换,d)任选地在步骤c)之前蒸汽成型催化剂,至少在步骤d)的蒸汽和蒸 的步骤a)一个是强制性的,e)在催化剂上引入磷以引入至少0.1重量%的磷,所述引入通过干浸渍或化学气相沉积制成,f)任选地引入 任选地与步骤e)同时处理金属,g)任选地洗涤催化剂,h)任选地煅烧催化剂,i)蒸煮催化剂,也称为平衡步骤。 在第二个实施方案中,磷可以通过任何方式引入,并且步骤i)蒸汽的苛刻度(X)至少约为2.在所述第二实施方案中,有利地,催化剂在高于625℃,优选在700℃ 至800°C。 步骤f)的金属有利地是钙。