会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 3. 发明授权
    • Melt-processable block copolyesterimide and method for manufacturing it
    • 熔融加工性嵌段共聚酯酰亚胺及其制造方法
    • US5677394A
    • 1997-10-14
    • US406859
    • 1995-04-28
    • Frank BohmeDoris PospiechManfred RatzschChrister BergstromMika HarkonenHeli AlankoPentti Passiniemi
    • Frank BohmeDoris PospiechManfred RatzschChrister BergstromMika HarkonenHeli AlankoPentti Passiniemi
    • C08J5/18B29C45/00B29C47/00B29C49/00B29D22/00B29D23/00B29D99/00B29K79/00C08G63/685C08G73/16C08L79/08
    • C08G73/16C08G63/685C08L79/08
    • A melt-processable block copolyesterimide comprising the repeating units (I), (II) and (III) and, optionally, a repeating unit (IV), wherein (I) is a repeating unit of the formula ##STR1## wherein R is an aliphatic polyether chain and/or a polysiloxane chain; (II) and (III) are repeating units of the formulas ##STR2## wherein Z is hydrogen, alkyl, alkoxy, aryl, halogen and w is zero or one; and (IV) is a repeating unit of the formula ##STR3## wherein Z' is hydrogen, alkyl, alkoxy, aryl or halogen and the phenylene ring is substituted in by Z' in the m- or p-positions. The repeating unit of formula (I) is present in an amount of 5 to 50 mole-%, the repeating unit of formula (II) is present in an amount of 10 to 80 mole-%, the repeating unit of formula (III) is present in an mount of 5 to 50 mole-% and the repeating unit of formula (IV) is present in an amount of 0 to 45 mole-% of the block copolyesterimide. The polymer according to the invention has liquid crystalline properties and it can be used as thermoplastic elastomer component of polymer compounds.
    • PCT No.PCT / FI93 / 00374 Sec。 371日期:1995年4月28日 102(e)1995年4月28日PCT PCT 1993年9月17日PCT公布。 公开号WO94 / 06846 日期1994年3月31日包含重复单元(I),(II)和(III)的可熔融加工的嵌段共聚酯酰亚胺和任选的重复单元(IV),其中(I)是下式的重复单元:IMAGE >(I)其中R是脂族聚醚链和/或聚硅氧烷链; (II)和(III)是式(III)的重复单元,其中Z是氢,烷基,烷氧基,芳基,卤素,w是0或1; 和(IV)是式(IV)的重复单元,其中Z'是氢,烷基,烷氧基,芳基或卤素,并且亚苯基环被m'或p-位上的Z'取代。 式(I)的重复单元以5至50摩尔%的量存在,式(II)的重复单元的存在量为10至80摩尔%,式(III)的重复单元 以5至50摩尔%的含量存在,并且式(IV)的重复单元以嵌段共聚酯酰亚胺的0至45摩尔%的量存在。 根据本发明的聚合物具有液晶性质,并且可以用作聚合物化合物的热塑性弹性体组分。
    • 8. 发明申请
    • Method for curing aminoplasts
    • 固化氨基塑料的方法
    • US20060084007A1
    • 2006-04-20
    • US10517963
    • 2003-06-12
    • Manfred RatzschHartmut BuckaMartin BurgerUwe Muller
    • Manfred RatzschHartmut BuckaMartin BurgerUwe Muller
    • G03C1/76D02G3/00F16J15/20
    • D01F6/76C08K5/18C08K5/3492C08K5/42C08L61/28C09D161/28Y10T428/2913Y10T428/2915C08L61/00
    • A method for curing aminoplasts, during which layers having layer thicknesses of up to 300 um or filaments and fiber fibrids having a diameter of up to 300 um, which consist of: i) 95 to 99.95% by mass of solvent-free meltable aminoplast polycondensates with molar masses ranging from 1000 to 300000; j) 5 to 0.05% by mass of curing agents, which can be activated by actinic light and which are comprised of acidifiers of the blocked sulfonic acid and/or halogen-substituted triazine derivative and/or onium salt type, and optionally; k) 1 to 20% by mass, with regard to the meltable aminoplast polycondensates, of unmodified and/or modified maleic anhydride copolymers, and/or; i) 0.1 to 5% by mass, with regard to the meltable aminoplast polycondensates, of nanoparticles. The aminoplasts are cured by irradiating them with actinic light at a temperature between the melting point of the aminoplast polycondensate and the thermoinduced decomposition temperature of the light-activatable curing agents. This method enables the production of, preferably, textile fabrics or coatings.
    • 一种用于固化氨基塑料的方法,其中具有高达300μm的层厚度或直径高达300μm的长丝和纤维纤维素,其由以下组成:i)95至99.95质量%的无溶剂的可熔化氨基塑料缩聚物 摩尔质量范围为1000〜300000; j)5〜0.05质量%的固化剂,其可以通过光化剂活化,并且其由阻断的磺酸和/或卤素取代的三嗪衍生物和/或鎓盐型的酸化剂和任选的; k)1〜20质量%,相对于可熔融的氨基塑料缩聚物,未改性和/或改性的马来酸酐共聚物,和/或; i)相对于可熔化氨基塑料缩聚物,为0.1〜5质量%的纳米粒子。 通过在氨基塑料缩聚物的熔点和可光活化的固化剂的热分解温度之间的温度下用光化光照射氨基塑料来固化。 该方法能够生产优选的织物或涂层。