    • 배진용최규범송수정이동근임호섭
    • C08G64/30C08G64/04C08K5/51C08L69/00
    • C08G64/083C08G64/14C08G64/307
    • A manufacturing method for branched polycarbonate of the present invention comprises: a step of manufacturing a first raw material by mixing an aromatic dihydroxy compound, diarylcarbonate and 60-140 ppb (weight) of a catalyst with respect to the aromatic dihydroxy compound and reacting the same; a step of manufacturing a second raw material by mixing an aromatic dihydroxy compound, diarylcarbonate, a phosphorus based branching agent and 350-450 ppb (weight) of a catalyst with respect to the aromatic dihydroxy compound and reacting the same; and a step of performing melt polymerization on 100 parts by weight of the first raw material and 1-20 parts by weight of the second raw material. The branched polycarbonate manufactured by the manufacturing method has excellent thermal stability since catalyst content is low and exhibits excellent color stability and mobility.
    • 本发明的支链聚碳酸酯的制造方法包括:通过将芳族二羟基化合物,二芳基碳酸酯和60-140ppb(重量)的催化剂相对于芳族二羟基化合物混合并使其反应来制造第一原料的步骤 ; 通过将芳族二羟基化合物,碳酸二芳基酯,磷基支化剂和相对于芳族二羟基化合物的350-450ppb(重量)的催化剂混合并使其反应来制造第二原料的步骤; 以及对第一原料100重量份和第二原料1-20重量份进行熔融聚合的工序。 通过制造方法制造的支化聚碳酸酯由于催化剂含量低而具有优异的热稳定性,并表现出优异的颜色稳定性和迁移率。
    • 5. 发明公开
    • 분지형 폴리카보네이트 수지 및 그 제조방법
    • 高分子量聚碳酸酯树脂及其制备方法
    • KR1020140019637A
    • 2014-02-17
    • KR1020120086013
    • 2012-08-06
    • 제일모직주식회사
    • 임호섭최규범배진용장복남
    • C08G64/04C08G64/20C08L69/00
    • C08G64/083C08G64/14
    • A polycarbonate resin in the present invention is polymerized by a branching agent repregented by chemical formula 2, Mark-Houwink constant thereof is 0.4-0.60, and the concentration of a terminal hydroxyl group is 22% of total terminal groups. The branched polycarbonate resin remarkably decreases the concentration of hydroxyl groups so yellowness is improved and highly branched structure can be obtained. In the chemical formula 1, each of R1, R2, R3, and R4 is independently a substituted or non-substituted C1-10 alkyl group, a substituted or non-substituted C6-C18 aryl group, a C1-C10 alkyl group with halogen or a C1-C10 alkoxy group, or a C6-C18 aryl group with halogen or a C1-C10 alkoxy group substituent; W is a linear, branched, or cyclic saturated or unsaturated hydrocarbon group, saturated or unsaturated cyclic hydrocarbon substituent-containing hydro carbon group, an O or S-containing hydro carbon group, or S.
    • 本发明的聚碳酸酯树脂通过化学式2表示的支化剂聚合,Mark-Houwink常数为0.4〜0.60,末端羟基的浓度为总末端的22%。 支链聚碳酸酯树脂显着降低羟基的浓度,因此改善了黄色度并且可以获得高度支化的结构。 在化学式1中,R 1,R 2,R 3和R 4各自独立地为取代或未取代的C 1-10烷基,取代或未取代的C 6 -C 18芳基,具有卤素的C 1 -C 10烷基 或C 1 -C 10烷氧基,或具有卤素或C 1 -C 10烷氧基取代基的C 6 -C 18芳基; W是直链,支链或环状饱和或不饱和烃基,含饱和或不饱和环烃基取代基的烃基,含O或S的氢碳基团或S.