    • METHOD OF PRODUCING A MULTILAYER MICROELECTRONIC SUBSTRATE
    • 生产多层微电子基板的方法
    • WO2003043035A1
    • 2003-05-22
    • PCT/IB2002/004763
    • 2002-11-13
    • KONINKLIJKE PHILIPS ELECTRONICS N.V.PHILIPS CORPORATE INTELLECTUAL PROPERTY GMBHZASPALIS, VassiliosBOEREKAMP, Jacobus, G.
    • ZASPALIS, VassiliosBOEREKAMP, Jacobus, G.
    • H01F41/02
    • H01F41/02H01F41/046H05K1/0306H05K1/162H05K1/165H05K3/4611H05K3/4629
    • A method of producing a multilayer microelectronic substrate, in which: a) a number of thermally combinable films with a first compression temperature are provided; b) at least one film with a second compression temperature, which lies above the first compression temperature, is provided; c) at least one of the films with the second compression temperature is arranged between films with the first compression temperature; d) the laminated films are heated to the first compression temperature, and further to a first end-temperature until the films with the first compression temperature are completely compressed, the first end-temperature being kept below the second compression temperature; and e) the laminated films are heated to the second compression temperature and, if applicable, further to a second end-temperature in order to compress the at least one film with the second compression temperature, characterized in that at least one of the films is made from magnetodielectric material, with nickel oxide NiO and ferrous oxide Fe 2 O 3 as the main components of a ferrite which contains bismuth oxide Bi 2 O 3 or a eutectic mixture of lead oxide PbO and at least one further metallic oxide or of bismuth oxide Bi 2 O 3 and at least one further metallic oxide.
    • 一种制造多层微电子衬底的方法,其中:a)提供多个具有第一压缩温度的可热组合膜; b)提供具有高于第一压缩温度的第二压缩温度的至少一个膜; c)具有第二压缩温度的膜中的至少一个被布置在具有第一压缩温度的膜之间; d)将层压膜加热到第一压缩温度,并进一步达到第一端温,直到具有第一压缩温度的膜被完全压缩,第一端温度保持在第二压缩温度以下; 以及e)层压膜被加热到第二压缩温度,如果适用,进一步加热到第二终止温度,以便以第二压缩温度压缩至少一个膜,其特征在于,至少一个膜是 由氧化镍NiO和氧化亚铁Fe 2 O 3作为铁氧体的主要成分,其含有氧化铋Bi 2 O 3或氧化铅PbO和至少一种其它金属氧化物或氧化铋Bi 2 O 3的共晶混合物,以及至少一种另外的氧化铋 金属氧化物。