基本信息:
- 专利标题: METHOD OF MAKING POLYBENZIMIDAZOLE
- 专利标题(中):制备聚苯并咪唑的方法
- 申请号:PCT/US2014/040590 申请日:2014-06-03
- 公开(公告)号:WO2014197413A1 公开(公告)日:2014-12-11
- 发明人: BENICEWICZ, Brian, C. , GULLEDGE, Alexander, Lanier , STECKLE, Jr., Warren, P. , COPELAND, Gregory, S. , DAWKINS, Bobby, G.
- 申请人: PBI PERFORMANCE PRODUCTS, INC.
- 申请人地址: 9800-D Southern Pine Boulevard Charlotte, NC 28273 US
- 专利权人: PBI PERFORMANCE PRODUCTS, INC.
- 当前专利权人: PBI PERFORMANCE PRODUCTS, INC.
- 当前专利权人地址: 9800-D Southern Pine Boulevard Charlotte, NC 28273 US
- 代理机构: HAMMER III, Robert, H. et al.
- 优先权: US61/830,869 20130604; US14/293,211 20140602
- 主分类号: C08G73/18
- IPC分类号: C08G73/18
摘要:
A method of making a polybenzimidazole (PBI) includes the steps of: reacting, in a solution, an organic compound having at least 2 amino groups with an organic aldehyde adduct, the reactants comprise at least 8% by weight of the solution. A solvent of the solution may be selected from the group of: N, N-dimethylacetamide (DMAc), N, N-dimethylformamide (DMF), dimethylsulfoxide (DMSO), N-methyl-2-pyrrolidone (NMP), tetramethylene sulfone, and combinations thereof. The organic aldehyde adduct may be an organic aldehyde bisulfite adduct. The organic aldehyde portion of the organic aldehyde adduct being aliphatic, alicyclic, aromatic, heterocyclic, or heteroaromatic aldehyde or mixtures thereof. The polybenzimidazole may have an intrinsic viscosity of at least 0.40 dl/g.
摘要(中):
制备聚苯并咪唑(PBI)的方法包括以下步骤:在溶液中使具有至少2个氨基的有机化合物与有机醛加合物反应,反应物包含至少8重量%的溶液。 该溶液的溶剂可以选自N,N-二甲基乙酰胺(DMAc),N,N-二甲基甲酰胺(DMF),二甲基亚砜(DMSO),N-甲基-2-吡咯烷酮(NMP),四亚甲基砜, 及其组合。 有机醛加合物可以是有机醛亚硫酸氢盐加合物。 有机醛加合物的有机醛部分是脂族,脂环族,芳族,杂环或杂芳族醛或其混合物。 聚苯并咪唑的特性粘度可以至少为0.40dl / g。
IPC结构图谱:
C | 化学;冶金 |
--C08 | 有机高分子化合物;其制备或化学加工;以其为基料的组合物 |
----C08G | 用碳—碳不饱和键以外的反应得到的高分子化合物 |
------C08G73/00 | 不包括在C08G12/00到C08G71/00组内的,在高分子主链中形成含氮的键合,有或没有氧或碳键合反应得到的高分子化合物 |
--------C08G73/02 | .聚胺 |
----------C08G73/18 | ..聚苯并咪唑 |