基本信息:
- 专利标题: SOLID CERAMIC ELECTROLYTES
- 专利标题(中):固体陶瓷电解液
- 申请号:PCT/US2013/070288 申请日:2013-11-15
- 公开(公告)号:WO2014078648A1 公开(公告)日:2014-05-22
- 发明人: BROWN, Jacqueline Leslie
- 申请人: CORNING INCORPORATED , BROWN, Jacqueline Leslie
- 申请人地址: 1 Riverfront Plaza Corning, New York 14831 US
- 专利权人: CORNING INCORPORATED,BROWN, Jacqueline Leslie
- 当前专利权人: CORNING INCORPORATED,BROWN, Jacqueline Leslie
- 当前专利权人地址: 1 Riverfront Plaza Corning, New York 14831 US
- 代理机构: RUSSELL, Michael W
- 优先权: US13/677,654 20121115
- 主分类号: H01M12/06
- IPC分类号: H01M12/06 ; C01F7/00 ; C04B35/447 ; B25B9/00 ; G01N27/406 ; H01M10/0525 ; H01M10/0562
摘要:
A solid ceramic electrolyte may include an ion-conducting ceramic and at least one grain growth inhibitor. The ion-conducting ceramic may be a lithium metal phosphate or a derivative thereof. The grain growth inhibitor may be magnesia, titania, or both. The solid ceramic electrolyte may have an average grain size of less than about 2 microns. The grain growth inhibitor may be between about 0.5 mol.% to about 10 mol.% of the solid ceramic electrolyte.
摘要(中):
固体陶瓷电解质可以包括离子导电陶瓷和至少一种晶粒生长抑制剂。 离子导电陶瓷可以是磷酸锂金属或其衍生物。 晶粒生长抑制剂可以是氧化镁,二氧化钛或二者。 固体陶瓷电解质可以具有小于约2微米的平均粒度。 晶粒生长抑制剂可以在固体陶瓷电解质的约0.5mol%至约10mol%之间。
IPC结构图谱:
H | 电学 |
--H01 | 基本电气元件 |
----H01M | 用于直接转变化学能为电能的方法或装置,例如电池组 |
------H01M12/00 | 混合电池;及其制造 |
--------H01M12/04 | .由燃料电池型的半电池和一次电池型的半电池组成的 |
----------H01M12/06 | ..带有一个金属电极和一个气体电极的 |