- 专利标题: POLYALPHAOLEFINS BY OLIGOMERIZATION AND ISOMERIZATION
- 专利标题(中):通过低聚和异构化制备聚异戊二烯
- 申请号:PCT/US2012/026865 申请日:2012-02-28
- 公开(公告)号:WO2012134688A1 公开(公告)日:2012-10-04
- 发明人: WU, Margaret, M. , PAFFORD, Bernie, J. , STAVENS, Kevin, B.
- 申请人: EXXONMOBIL CHEMICAL PATENTS INC. , WU, Margaret, M. , PAFFORD, Bernie, J. , STAVENS, Kevin, B.
- 申请人地址: A Corporation Of The State Of Delaware 5200 Bayway Drive Baytown, TX 77520-2101 US
- 专利权人: EXXONMOBIL CHEMICAL PATENTS INC.,WU, Margaret, M.,PAFFORD, Bernie, J.,STAVENS, Kevin, B.
- 当前专利权人: EXXONMOBIL CHEMICAL PATENTS INC.,WU, Margaret, M.,PAFFORD, Bernie, J.,STAVENS, Kevin, B.
- 当前专利权人地址: A Corporation Of The State Of Delaware 5200 Bayway Drive Baytown, TX 77520-2101 US
- 代理机构: KRAWCZYK, Nancy, T. et al.
- 优先权: US61/469,457 20110330
- 主分类号: C10G50/02
- IPC分类号: C10G50/02 ; C08F10/00 ; C08F10/14 ; C10M107/10
摘要:
A feedstock of one or more C4 to C24 alpha olefins is oligomerized with a metallocene catalyst system to form a polyalphaolefin product mixture. At least a portion of the polyalphaolefin product mixture is then isomerized in the presence of an acid catalyst to form an isomerized polyalphaolefin. The polyalphaolefin may also by hydrogenated, either simultaneously with isomerization or afterwards. The resulting polyalphaolefin has a kinematic viscosity at 100°C of between 1 cSt and 20 cSt and reduced pour point in comparison to the pre-isomerized product.
摘要(中):
一种或多种C 4至C 24α-烯烃的原料用茂金属催化剂体系低聚以形成聚α-烯烃产物混合物。 然后将至少一部分聚α-烯烃产物混合物在酸催化剂存在下异构化以形成异构化的聚α烯烃。 聚α-烯烃也可以通过氢化,同时异构化或之后。 得到的聚α烯烃在100℃下的运动粘度在1cSt和20cSt之间,与预异构化产物相比具有降低的倾点。