发明申请
WO02008478A1 A METHOD OF PRODUCING A CERAMIC BODY BY COALESCENCE AND THE CERAMIC BODY PRODUCED
审中-公开
基本信息:
- 专利标题: A METHOD OF PRODUCING A CERAMIC BODY BY COALESCENCE AND THE CERAMIC BODY PRODUCED
- 专利标题(中):通过煤炭生产陶瓷体的方法和生产的陶瓷体
- 申请号:PCT/SE2001/001673 申请日:2001-07-25
- 公开(公告)号:WO02008478A1 公开(公告)日:2002-01-31
- 主分类号: A61L27/00
- IPC分类号: A61L27/00 ; A61L27/42 ; A61L27/44 ; B22F3/087 ; B22F3/17 ; B22F7/06 ; B28B3/02 ; B29C43/00 ; B29C43/14 ; B29C43/16 ; B29C43/32 ; B29K23/00 ; B29K33/04 ; B29K103/00 ; B29K105/16 ; B29L31/00 ; B30B11/00 ; B30B11/02 ; C22C1/05 ; C22C1/04 ; B21J5/00 ; B22F3/02 ; C22C29/00
摘要:
A method of producing a ceramic body by coalescence, wherein the method comprises the steps of a) filling a pre-compacting mould with ceramic material in the form of powder, pellets, grains and the like, b) pre-compacting the material at least once and c) compressing the material in a compression mould by at least one stroke, where a striking unit emits enough kinetic energy to form the body when striking the material inserted in the compression mould, causing coalescence of the material. A method of producing a ceramic body by coalescence, wherein the method comprises compressing material in the form of a solid ceramic body in a compression mould by at least one stroke, where a striking unit emits enough energy to cause coalescence of the material in the body.Products obtained by the inventive methods.
摘要(中):
一种通过聚结生产陶瓷体的方法,其中所述方法包括以下步骤:a)用粉末,粒料,颗粒等形式的陶瓷材料填充预压模; b)至少预压制材料 一次并且c)将压缩模具中的材料压缩至少一个行程,其中打击单元在撞击插入压缩模具中的材料时发出足够的动能以形成身体,从而引起材料的聚结。 一种通过聚结生产陶瓷体的方法,其中所述方法包括以至少一个冲程在压缩模具中压制固体陶瓷体形式的材料,其中击打单元发射足够的能量以引起材料在体内的聚结 通过本发明方法获得的产品。
IPC结构图谱:
A | 人类生活必需 |
--A61 | 医学或兽医学;卫生学 |
----A61L | 材料或物体消毒的一般方法或装置;空气的灭菌、消毒或除臭;绷带、敷料、吸收垫或外科用品的化学方面;绷带、敷料、吸收垫或外科用品的材料 |
------A61L27/00 | 假体材料或假体被覆材料 |