基本信息:
- 专利标题: Wellbore Servicing Materials and Methods of Making and Using Same
- 专利标题(中):Wellbore维修材料及其使用方法
- 申请号:US13856734 申请日:2013-04-04
- 公开(公告)号:US20140303046A1 公开(公告)日:2014-10-09
- 发明人: Dipti SINGH , B. Raghava REDDY , Jeremy HOLTSCLAW
- 申请人: HALLIBURTON ENERGY SERVICES, INC.
- 申请人地址: US TX Houston
- 专利权人: Halliburton Energy Services, Inc.
- 当前专利权人: Halliburton Energy Services, Inc.
- 当前专利权人地址: US TX Houston
- 主分类号: C09K8/90
- IPC分类号: C09K8/90
摘要:
A method of servicing a wellbore in a subterranean formation comprising placing a wellbore servicing fluid in the wellbore and/or subterranean formation, wherein the wellbore servicing fluid comprises a viscosifying polymeric material, a breaking agent comprising an inorganic peroxide of a divalent metal M(II) characterized by the general formula MO2, and a break rate controlling additive comprising a M(II) soluble salt, a M(II) precipitating salt, a M(II) surface precipitating salt, a M(II) solution precipitating salt, or combinations thereof, allowing the wellbore servicing fluid to break, and flowing back to the surface at least a portion of the broken wellbore servicing fluid.
摘要(中):
一种维护地下地层中的井眼的方法,包括将井眼维修流体放置在井筒和/或地下地层中,其中井筒维修流体包括增粘聚合材料,包含二价金属M(II)的无机过氧化物的破坏剂 (II)可溶性盐,M(II)沉淀盐,M(II)表面沉淀盐,M(II)溶液沉淀盐或者(II))沉淀盐的断裂速率控制添加剂,或 允许井筒维修流体破裂,并将破裂的井眼维修流体的至少一部分流回表面。
公开/授权文献:
IPC结构图谱:
C | 化学;冶金 |
--C09 | 染料;涂料;抛光剂;天然树脂;黏合剂;其他类目不包含的组合物;其他类目不包含的材料的应用 |
----C09K | 不包含在其他类目中的各种应用材料;不包含在其他类目中的材料的各种应用 |
------C09K8/00 | 用于钻孔或钻井的组合物;用来处理孔或井的组合物,例如,用于完成或修复操作 |
--------C09K8/56 | .用于固定井四周的散沙或类似物但不会过度降低其渗透性的组合物 |
----------C09K8/84 | ..水基或极性溶剂组合物 |
------------C09K8/86 | ...含有有机化合物 |
--------------C09K8/88 | ....高分子化合物 |
----------------C09K8/90 | .....来自天然原料,例如多糖、纤维素 |