摘要:
A catalyst composition that has superior attrition performance and a method that produces said catalyst composition to be used for fluid catalytic cracking processes to convert a heavy hydrocarbon fraction into mainly liquid fuels, particularly gasoline and light olefins. The catalyst composition has a moisture level or loss on ignition below 12 wt % and attrition rate below 3 wt. %/hr.
摘要(中):
具有优异的磨耗性能的催化剂组合物和产生用于流化催化裂化方法的所述催化剂组合物以将重质烃馏分转化成主要是液体燃料,特别是汽油和轻质烯烃的方法。 催化剂组合物具有低于12重量%的水分含量或灼烧损失,并且磨耗率低于3重量%。 %/小时。