发明申请
US20060106179A1 Methods of preparing EP(D)M elastomer, of controlling yield thereof, and of recovering the same
有权
![Methods of preparing EP(D)M elastomer, of controlling yield thereof, and of recovering the same](/abs-image/US/2006/05/18/US20060106179A1/abs.jpg.150x150.jpg)
基本信息:
- 专利标题: Methods of preparing EP(D)M elastomer, of controlling yield thereof, and of recovering the same
- 专利标题(中):制备EP(D)M弹性体,控制其收率和回收其的方法
- 申请号:US11138072 申请日:2005-05-26
- 公开(公告)号:US20060106179A1 公开(公告)日:2006-05-18
- 发明人: Sang Kim , Hee Koo
- 申请人: Sang Kim , Hee Koo
- 优先权: KR2004-94750 20041118
- 主分类号: C08F36/00
- IPC分类号: C08F36/00
摘要:
Disclosed herein is a method of preparing an EP(D)M elastomer, which includes pre-cooling a reactive solvent to −80 to −100° C.; and polymerizing ethylene, at least one higher α-olefin having 3 to 18 carbons, and selectively, at least one conjugated or non-conjugated diene having 5 to 15 carbons, in the presence of the reactive solvent. According to the method of the current invention, the yield of the EP(D)M elastomer is drastically increased even though a conventional preparation device is used unchanged. Further, methods of controlling the yield of the EP(D)M elastomer and of recovering the EP(D)M elastomer are provided.
摘要(中):
本文公开了制备EP(D)M弹性体的方法,其包括将反应性溶剂预冷至-80至-100℃; 并在反应性溶剂的存在下使乙烯,至少一种具有3至18个碳原子的高级α-烯烃和选择性地至少一种具有5至15个碳原子的共轭或非共轭二烯聚合。 根据本发明的方法,即使使用常规的制备装置不变,EP(D)M弹性体的收率也急剧增加。 此外,提供了控制EP(D)M弹性体的收率和回收EP(D)M弹性体的方法。