基本信息:
- 专利标题: 고장력 강판 및 그 제조방법
- 专利标题(英):KR102237628B1 - High-strength steel sheet and method of manufacturing the same
- 申请号:KR1020190104165 申请日:2019-08-26
- 公开(公告)号:KR102237628B1 公开(公告)日:2021-04-07
- 发明人: 정유담 , 박진성
- 申请人: 현대제철 주식회사
- 申请人地址: 인천광역시 동구...
- 专利权人: 현대제철 주식회사
- 当前专利权人: 현대제철 주식회사
- 当前专利权人地址: 인천광역시 동구...
- 代理人: 특허법인아주
- 主分类号: C22C38/38
- IPC分类号: C22C38/38 ; C22C38/26 ; C22C38/28 ; C21D8/02 ; B21C47/06
A method of manufacturing a high-tensile steel sheet according to an aspect of the present invention is in weight%, carbon (C): 0.10 to 0.30%, silicon (Si): 0.1 to 1.0%, manganese (Mn): 1.50 to 2.70%, phosphorus (P) ): more than 0 and less than 0.02%, sulfur (S): more than 0 and less than 0.003%, soluble aluminum (Al): 0.01 to 0.10%, chromium (Cr): 0.1 to 1.0%, niobium (Nb): 0.01 to 0.05%, Titanium (Ti): 0.001 ~ 0.05%, boron (B): 0.0001 ~ 0.004%, nitrogen (N): more than 0 0.0060% or less Reheating the steel slab containing the remaining iron (Fe) and other inevitable impurities; Obtaining a hot-rolled sheet by hot finish rolling the reheated steel slab at AC3 ~ 960°C; And cooling the hot-rolled sheet material to a winding temperature: 420 to 650°C, and then winding it.
公开/授权文献:
- KR1020210024709A 고장력 강판 및 그 제조방법 公开/授权日:2021-03-08
信息查询:
EspacenetIPC结构图谱:
C | 化学;冶金 |
--C22 | 冶金(铁的冶金入C21);黑色或有色金属合金;合金或有色金属的处理 |
----C22C | 合金 |
------C22C38/00 | 铁基合金,例如合金钢 |
--------C22C38/18 | .含铬的 |
----------C22C38/38 | ..含大于1.5(重量)的锰 |