基本信息:
- 专利标题: 용융 아연 도금 강판
- 专利标题(英):Hot-dip galvanized steel sheet
- 专利标题(中):热浸镀锌钢板
- 申请号:KR1020177010984 申请日:2015-11-05
- 公开(公告)号:KR1020170063785A 公开(公告)日:2017-06-08
- 发明人: 가와타히로유키 , 야스이다케시 , 우에다고헤이 , 마루야마나오키 , 야마구치유지 , 우치다사토시 , 고마미료스케 , 아라이하야토 , 나카무라도요미츠
- 申请人: 신닛테츠스미킨 카부시키카이샤
- 申请人地址: *-*, Marunouchi *-chome, Chiyoda-ku, Tokyo, Japan
- 专利权人: 신닛테츠스미킨 카부시키카이샤
- 当前专利权人: 신닛테츠스미킨 카부시키카이샤
- 当前专利权人地址: *-*, Marunouchi *-chome, Chiyoda-ku, Tokyo, Japan
- 代理人: 양영준; 최인호; 성재동
- 优先权: JPJP-P-2014-225525 2014-11-05
- 国际申请: PCT/JP2015/081237 2015-11-05
- 国际公布: WO2016072479 2016-05-12
- 主分类号: C23C2/06
- IPC分类号: C23C2/06 ; C23C2/26 ; C23C2/40 ; C23C2/02 ; C22C38/02 ; C22C38/06 ; C22C38/04 ; C22C38/58 ; C21D9/46
It includes a base steel sheet and hot-dip galvanizing layer, and a ferrite phase and 50% or less, the hard tissue at least 50% by volume fraction in the range of 1/8 to 3/8 the thickness from the thickness of the base metal steel sheet surface, starting from the interface between the plated layer and the base material steel plate a base material with a volume fraction of the retained austenite volume fraction of 3% or less nitro, hard tissue within the range of the steel sheet to a depth 20㎛ to, 1/8 the thickness to 0.10 to 0.90 times the volume fraction of a base material in the thickness range of 3/8 on the surface of the steel sheet, Fe: 5% or less, Al: 1.0% or less, having a hot-dip galvanizing layer on and through the main-phase crystal containing the ζ phase to at least 20% of the interface between the plated layer and the steel sheet of the base metal steel sheet surface side to have a fine layer, the average grain size of the ferrite in the average thickness of the finer layer, finely divided layer, the maximum diameter of the oxide is individually hot-dip galvanized steel sheet defined as included in the refinement layer.
公开/授权文献:
- KR101913986B1 용융 아연 도금 강판 公开/授权日:2018-10-31