基本信息:
- 专利标题: 경도를 강화시킨 숯의 제조방법과, 숯검정억제 및내마모성을 갖는 숯 및 이의 제조방법
- 专利标题(英):Method for fabricating solid charcoal solidified hardness, a uncolored and solid charcoal and method for fabricating thereof
- 专利标题(中):制造硬度增强材料的方法,特殊用途抑制和磨蚀电阻煤及其制造方法
- 申请号:KR1020000060020 申请日:2000-10-12
- 公开(公告)号:KR1020020029197A 公开(公告)日:2002-04-18
- 发明人: 염충렬
- 申请人: 조재현
- 申请人地址: 경기도 시흥시 목감초등길 *, 삼호가든아파트 ***동 ***호 (조남동)
- 专利权人: 조재현
- 当前专利权人: 조재현
- 当前专利权人地址: 경기도 시흥시 목감초등길 *, 삼호가든아파트 ***동 ***호 (조남동)
- 代理人: 특허법인정직과특허; 이희명
- 主分类号: C10B57/02
- IPC分类号: C10B57/02
摘要:
PURPOSE: A method for manufacturing a hardness reinforced charcoal which can be fabricated into accessories so that charcoal useful to the human body contacts the body and is used in water purification, a charcoal soot inhibiting and abrasion resisting coal and a method for manufacturing the same are provided. CONSTITUTION: The method for manufacturing a hardness reinforced charcoal comprises a first step(S10) of preparing wood; a second step(S20) of heating the wood in the temperature range of 600 to 800 deg.C after putting the wood into a closed kiln; a third step(S30) of heating an internal temperature of the kiln in the temperature range of 1000 to 1300 deg.C by partially opening the kiln after a certain period of time, thereby supplying air into the kiln; a fourth step(S40) of cutting a resulting material of the third step; a fifth step(S50) of processing the resulting material of the fourth step into a shape selected from a ring shape, a polygonal plate shape, a polygonal cylinder shape and a pyramid shape; a sixth step(S60) of cleaning the resulting material in boiling water so as to discharge charcoal powder from charcoal pores after cleaning the resulting material until generation of charcoal powder is inhibited from the resulting material of the fifth step; and a seventh step(S70) of drying the resulting material of the sixth step.
摘要(中):
目的:制造硬质增强木炭的方法,其可以制成附件,使得对人体有用的木炭与身体接触并用于水净化,木炭烟灰抑制和耐磨煤及其制造方法。 提供。 构成:制造硬度增强的木炭的方法包括制备木材的第一步(S10) 在将木材放入封闭的窑内之后,在600〜800℃的温度范围内对木材进行加热的第二工序(S20) 第三步骤(S30),通过在一定时间段之后部分地打开窑来在1000〜1300℃的温度范围内加热窑的内部温度,从而向窑内供给空气; 第四步骤(S40),切割第三步骤的所得材料; 将第四步骤的所得材料加工成从环形,多边形板状,多边形柱形和金字塔形形状的形状的第五步骤(S50) 第六步骤(S60),将所得材料在沸水中清洗,以在清洁所得材料之后将木炭粉末从活性炭孔中排出,直到产生的第五步骤产生的木炭粉末被抑制; 以及第七步骤(S70),其干燥所得到的第六步骤的材料。
信息查询:
EspacenetIPC结构图谱:
C | 化学;冶金 |
--C10 | 石油、煤气及炼焦工业;含一氧化碳的工业气体;燃料;润滑剂;泥煤 |
----C10B | 含碳物料的干馏生产煤气、焦炭、焦油或类似物 |
------C10B55/00 | 矿物油、沥青、焦油或类似物,或它们与固态含碳物料的混合物的焦化 |
--------C10B57/02 | .多步碳化或焦化工艺过程 |