基本信息:
- 专利标题: 고강도 Ti₃AlC₂ 복합재료 및 그 제조방법
- 专利标题(英):Ti3alc2 composite materials with high strength and manufacturing process of the same
- 专利标题(中):具有高强度和制造工艺的TI3ALC2复合材料
- 申请号:KR1020070126963 申请日:2007-12-07
- 公开(公告)号:KR100882924B1 公开(公告)日:2009-02-10
- 发明人: 박상환 , 한재호 , 윤성호 , 조경선
- 申请人: 한국과학기술연구원
- 申请人地址: 서울특별시 성북구 화랑로**길 * (하월곡동)
- 专利权人: 한국과학기술연구원
- 当前专利权人: 한국과학기술연구원
- 当前专利权人地址: 서울특별시 성북구 화랑로**길 * (하월곡동)
- 代理人: 백남훈; 이학수
- 主分类号: C04B35/478
- IPC分类号: C04B35/478 ; C04B35/56 ; B82Y30/00 ; B82Y40/00
摘要:
A high intensity of Ti3AlC2 is provided to have destructive strength measured by a three-point bending strength test method over 7000 MPa and to maintain excellent machinability, excellent thermal characteristic and excellent electrical characteristic. A high intensity of Ti3AlC2 composite includes Ti3AlC2, Ti2AlC and TiCy(y>0.6) to main crystal phase. The TiCy phase less than 100 nano size is strengthened in a Ti3AlC2 matrix phase. A content of Ti2AlC secondary phase included in the Ti3AlC2 matrix phase and non-reactive TiCy(y>0.6) is 10 volume % or less. A mean size of the Ti3AlC2 grain is 30 mum or less.
摘要(中):
提供高强度的Ti3AlC2以具有通过7000MPa的三点弯曲强度试验方法测量的破坏强度,并且保持优异的机械加工性,优异的热特性和优异的电特性。 高强度的Ti3AlC2复合材料包括主晶相的Ti3AlC2,Ti2AlC和TiCy(y> 0.6)。 在Ti3AlC2基体相中,小于100纳米尺寸的TiCi相增强。 包含在Ti 3 AlC 2基体相中的Ti 2 AlC第二相和非反应性TiC y(y> 0.6)的含量为10体积%以下。 Ti3AlC2晶粒的平均粒径为30μm以下。