High purity nickel by a simple means from the spent catalyst, cobalt, provides a method for recovering molybdenum, vanadium in high yield. The spent catalyst containing valuable metal is heated in a non-oxidizing atmosphere, deposition and a step of oil removal by thermal decomposition of the oil, spent catalyst and co-ground and chlorides deoiled, nickel and / or cobalt chloride and generating a spent catalyst that co-ground with water leach, oxidize the steps of dissolving nickel and / or cobalt in water, the leaching residue containing molybdenum and / or vanadium after water leaching, molybdenum and generating a / or oxides of vanadium, and alkaline leach leaching residue containing the oxides of molybdenum and / or vanadium, and a step of dissolving the molybdenum and / or vanadium in an alkaline solution, a.
公开/授权文献:
- JP5387851B2 Valuable metal recovery process from the waste catalyst 公开/授权日:2014-01-15
信息查询:
EspacenetIPC结构图谱:
C | 化学;冶金 |
--C22 | 冶金(铁的冶金入C21);黑色或有色金属合金;合金或有色金属的处理 |
----C22B | 金属的生产或精炼;原材料的预处理 |
------C22B7/00 | 处理非矿石原材料(如废料)以生产有色金属或其化合物 |