基本信息:
- 专利标题: Method of synthesizing trioxane in vapor phase
- 专利标题(中):在蒸气相中合成三氧化硫的方法
- 申请号:JP13363882 申请日:1982-08-02
- 公开(公告)号:JPS5925387A 公开(公告)日:1984-02-09
- 发明人: MATSUZAKI KAZUHIKO , MASAMOTO JIYUNZOU
- 申请人: Asahi Chem Ind Co Ltd
- 专利权人: Asahi Chem Ind Co Ltd
- 当前专利权人: Asahi Chem Ind Co Ltd
- 优先权: JP13363882 1982-08-02
- 主分类号: C07D323/06
- IPC分类号: C07D323/06 ; B01J23/00 ; B01J23/14 ; B01J23/20 ; B01J23/22 ; B01J23/28 ; B01J23/30 ; B01J27/00 ; B01J27/18 ; C07B61/00
摘要:
PURPOSE: To obtain the titled compound capable of giving high-molecular weight polyoxymethylene in high purity with little formation of by-products without depositing paraformaldehyde nor corroding apparatuses, by bringing formaldehyde in the vapor phase into contact with a heteropolyacid supported on a carrier.
CONSTITUTION: A carrier, e.g. silica gel, is gently agitated in an aqueous solution of a heteropolyacid, e.g. phosphotungstic acid, at 80°C, and the carrier is then separated and dried at 120°C under reduced pressure to afford a catalyst containing the heteropolyacid supported on the carrier. The resultant catalyst is then packed in a stainless steel tube, etc. having a jacket, the stainless steel tube, etc. and brought into contact with the catalyst consisting of the heteropolyacid supported on the carrier and give the aimed trioxane of high purity.
COPYRIGHT: (C)1984,JPO&Japio
摘要(中):
CONSTITUTION: A carrier, e.g. silica gel, is gently agitated in an aqueous solution of a heteropolyacid, e.g. phosphotungstic acid, at 80°C, and the carrier is then separated and dried at 120°C under reduced pressure to afford a catalyst containing the heteropolyacid supported on the carrier. The resultant catalyst is then packed in a stainless steel tube, etc. having a jacket, the stainless steel tube, etc. and brought into contact with the catalyst consisting of the heteropolyacid supported on the carrier and give the aimed trioxane of high purity.
COPYRIGHT: (C)1984,JPO&Japio
目的:通过使气相中的甲醛与负载在载体上的杂多酸接触,获得能够以高纯度产生高分子量聚甲醛的标题化合物,几乎不形成副产物而不沉积多聚甲醛或腐蚀装置。 构成:载体,例如 硅胶,在杂多酸的水溶液中轻轻搅拌,例如 磷钨酸,在80℃下,然后将载体分离并在120℃下减压干燥,得到含载体载体上的杂多酸的催化剂。 然后将得到的催化剂装入具有夹套,不锈钢管等的不锈钢管等中,并与负载在载体上的杂多酸组成的催化剂接触,得到高纯度的目标三恶烷。
公开/授权文献:
- JPS6337110B2 公开/授权日:1988-07-22
信息查询:
EspacenetIPC结构图谱:
C | 化学;冶金 |
--C07 | 有机化学 |
----C07D | 杂环化合物 |
------C07D323/00 | 杂环化合物,含多于两个氧原子作为仅有的杂环原子 |
--------C07D323/04 | .六元环 |
----------C07D323/06 | ..三烷 |