A no possible to use a complicated process and processing, such as without austempering the use of expensive chemical components, further selection and arrangement of the major chemical components extremely high levels of hardness and tensile by simple method obtaining a strength of the spherical graphite cast iron.
In A mass%, C: 3.0~4.0%, Si: 1.5~2.5%, Mn: 1.0% or less, P: 0.04% or less, S: 0. 0.3% or less, Mg: 0.02~0.1%, Cu: 1.8~3.3%, Sn: it contains 0.01 to 0.05 percent, the chemical composition of the balance Fe and unavoidable impurities in the melt, casting the Fe-Si by performing Si 0.05 to 0.15 wt% secondary inoculation eq performs give away early type when the austenitic state, spheroidal graphite cast iron, characterized in that for cooling the method of production.
.FIELD 1