摘要:
PROBLEM TO BE SOLVED: To provide a solidification material capable of solidifying an object to be solidified such as soft ground to a sufficient strength at a low cost, and to suppress hexavalent chromium contained in the object to be solidified such as cement and soil of the solidification material from being eluted from the object to be solidified after solidification.
SOLUTION: The solidification material contains cement, a waste plaster and a roast ash of an industrial waste produced by performing roasting under an atmosphere of a low concentration of oxygen at a temperature of 1,000-1,100°C. The cement is made to 25-45 wt.%, the waste plaster is made to 10-50 wt.% and the roast ash is made to 10-50 wt.%. More preferably, the cement is made to 30-40 wt.%, the waste plaster is made to 15-40 wt.% and the roast ash is made to 20-45 wt.%.
COPYRIGHT: (C)2008,JPO&INPIT
摘要(中):
SOLUTION: The solidification material contains cement, a waste plaster and a roast ash of an industrial waste produced by performing roasting under an atmosphere of a low concentration of oxygen at a temperature of 1,000-1,100°C. The cement is made to 25-45 wt.%, the waste plaster is made to 10-50 wt.% and the roast ash is made to 10-50 wt.%. More preferably, the cement is made to 30-40 wt.%, the waste plaster is made to 15-40 wt.% and the roast ash is made to 20-45 wt.%.
COPYRIGHT: (C)2008,JPO&INPIT
要解决的问题:提供一种能够以低成本固化待固化的物体如软土,以足够的强度固化的凝固材料,并且抑制待固化的物体中所含的六价铬,例如水泥和 凝固材料的土壤在固化后被固化的物体洗脱。 解决方案:固化材料含有水泥,废石膏和通过在低浓度氧气氛下在1000-1100℃的温度下进行焙烧而产生的工业废料的烤烟。 将水泥制成25-45重量%,将废石膏制成10-50重量%,并将焙烧粉制成10-50重量%。 更优选地,将水泥制成30-40重量%,将废石膏制成15-40重量%,并将焙烧粉制成20-45重量%。 版权所有(C)2008,JPO&INPIT
信息查询:
EspacenetIPC结构图谱:
C | 化学;冶金 |
--C09 | 染料;涂料;抛光剂;天然树脂;黏合剂;其他类目不包含的组合物;其他类目不包含的材料的应用 |
----C09K | 不包含在其他类目中的各种应用材料;不包含在其他类目中的材料的各种应用 |
------C09K17/00 | 土壤调节材料或土壤稳定材料 |
--------C09K17/02 | .只含无机化合物 |
----------C09K17/10 | ..水泥,如硅酸盐水泥 |