发明公开
EP4378998A1 POLYMER ALLOY, HOSE FOR HIGH-PRESSURE GAS, AND STORAGE CONTAINER FOR HIGH-PRESSURE GAS
审中-实审

基本信息:
- 专利标题: POLYMER ALLOY, HOSE FOR HIGH-PRESSURE GAS, AND STORAGE CONTAINER FOR HIGH-PRESSURE GAS
- 申请号:EP22849501.6 申请日:2022-07-26
- 公开(公告)号:EP4378998A1 公开(公告)日:2024-06-05
- 发明人: NISHI Eiichi , SASAKI Toru , TOKUMITSU Katsuhisa
- 申请人: AGC INC.
- 申请人地址: JP Chiyoda-ku, Tokyo 1008405 5-1, Marunouchi 1-chome,
- 专利权人: AGC INC.
- 当前专利权人: AGC INC.
- 当前专利权人地址: JP Chiyoda-ku, Tokyo 1008405 5-1, Marunouchi 1-chome,
- 代理机构: Müller-Boré & Partner Patentanwälte PartG mbB
- 优先权: JP 2021124230 2021.07.29
- 国际申请: JP2022028812 2022.07.26
- 国际公布: WO2023008440 2023.02.02
- 主分类号: C08L29/04
- IPC分类号: C08L29/04 ; C08F214/18 ; C08J5/04 ; C08L27/12 ; C08L77/00 ; F16J12/00 ; F16L11/04 ; F17C1/16 ; F17C13/00
摘要:
To provide a polymer alloy excellent in resistance to a high-pressure gas.
A polymer alloy, having a fluorinated copolymer having a carbonyl group-containing group, having a melting point of 250°C or lower, and at least one thermoplastic polymer selected from the group consisting of a polyamide and an ethylene/vinyl alcohol copolymer, immiscible with the fluorinated copolymer and having a melting point of 250°C or lower, melt-kneaded,
wherein the proportion of the fluorinated copolymer to the total mass of the polymer alloy is from 10 to 40 mass%, and
particles of the fluorinated copolymer are dispersed in the thermoplastic polymer, and the average particle size of the fluorinated copolymer particles in the polymer alloy is from 0.001 to 10 µm.
A polymer alloy, having a fluorinated copolymer having a carbonyl group-containing group, having a melting point of 250°C or lower, and at least one thermoplastic polymer selected from the group consisting of a polyamide and an ethylene/vinyl alcohol copolymer, immiscible with the fluorinated copolymer and having a melting point of 250°C or lower, melt-kneaded,
wherein the proportion of the fluorinated copolymer to the total mass of the polymer alloy is from 10 to 40 mass%, and
particles of the fluorinated copolymer are dispersed in the thermoplastic polymer, and the average particle size of the fluorinated copolymer particles in the polymer alloy is from 0.001 to 10 µm.