基本信息:
- 专利标题: INITIAL CRACK FORMATION METHOD
- 专利标题(中):初始裂纹形成方法
- 申请号:EP13852825.2 申请日:2013-11-01
- 公开(公告)号:EP2918558B1 公开(公告)日:2018-02-21
- 发明人: ITOH Sho , MORI Hiroki , MORI Koichi
- 申请人: Nippon Electric Glass Co., Ltd.
- 申请人地址: 7-1 Seiran 2-chome Otsu-shi Shiga 520-8639 JP
- 专利权人: Nippon Electric Glass Co., Ltd.
- 当前专利权人: Nippon Electric Glass Co., Ltd.
- 当前专利权人地址: 7-1 Seiran 2-chome Otsu-shi Shiga 520-8639 JP
- 代理机构: Tetzner, Michael
- 优先权: JP2012247230 20121109
- 国际公布: WO2014073472 20140515
- 主分类号: C03B33/037
- IPC分类号: C03B33/037 ; C03B33/023 ; C03B33/09 ; C03B33/10 ; B26D7/18 ; C03B33/03
摘要:
Provided is an initial crack formation device (1) for scoring a front-side end (Ga) in a conveyance direction (B) of a glass ribbon (G) conveyed by a belt conveyer (3) so as to form an initial crack group (CG) including a plurality of aggregated initial cracks (C) in a width direction of the front-side end (Ga) orthogonal to the conveyance direction (B). The initial crack formation device (1) includes a flap wheel (4) for scoring the front-side end (Ga) while rotating in a direction of drawing the glass ribbon (G) into the conveyance direction (B). The flap wheel (4) is configured to rotate at a rotational peripheral speed higher than a conveyance speed of the glass ribbon (G).
公开/授权文献:
- EP2918558A1 INITIAL CRACK FORMATION DEVICE, AND FORMATION METHOD 公开/授权日:2015-09-16
IPC结构图谱:
C | 化学;冶金 |
--C03 | 玻璃;矿棉或渣棉 |
----C03B | 制造、成型或辅助工艺 |
------C03B33/00 | 冷玻璃的裁割 |
--------C03B33/02 | .板玻璃的切割或分割;所用设备或机器 |
----------C03B33/023 | ..板处于水平位置 |
------------C03B33/037 | ...控制或调节 |