基本信息:
- 专利标题: PROCEDE DE MESURE DE LA TENACITE D'UN MATERIAU
- 专利标题(英):Method for measuring the tenacity of a material
- 专利标题(中):法测量材料的强度
- 申请号:EP13745421.1 申请日:2013-08-06
- 公开(公告)号:EP2883033A1 公开(公告)日:2015-06-17
- 发明人: ROUNTREE, Cindy , BONAMY, Daniel
- 申请人: Commissariat à l'Énergie Atomique et aux Énergies Alternatives
- 申请人地址: 25, rue Leblanc Bâtiment "Le Ponant D" 75015 Paris FR
- 专利权人: Commissariat à l'Énergie Atomique et aux Énergies Alternatives
- 当前专利权人: Commissariat à l'Énergie Atomique et aux Énergies Alternatives
- 当前专利权人地址: 25, rue Leblanc Bâtiment "Le Ponant D" 75015 Paris FR
- 代理机构: Brevalex
- 优先权: FR1257701 20120808
- 国际公布: WO2014023729 20140213
- 主分类号: G01N3/60
- IPC分类号: G01N3/60
摘要:
The invention relates to a method for measuring the tenacity K
c of a material, comprising the following steps: placing a sample of said material, having the shape of a parallelepiped rectangle through the middle of which a central hole extends, between two jaws of a clamping device, each of said jaws engaging with a distant end of the sample; moving the two jaws together so as to exert a force at each of said ends until the sample has completely broken; measuring the variations during the clamping on the basis of the time of the clamping force exerted at each end of the sample; determining the maximum value F
0 of said clamping force; marking three separate areas on the surface of one of the breaking surfaces, i.e. a first area close to the hole having a first type of embossment, a second area having a second type of embossment, and a third area having a third type of embossment that is less pronounced than the second type; measuring the distance L
0 between the edge of the hole and a transition line separating the second area from the third area; and calculating the parameter K
c on the basis of the force F
0 and distance L
0 .
c of a material, comprising the following steps: placing a sample of said material, having the shape of a parallelepiped rectangle through the middle of which a central hole extends, between two jaws of a clamping device, each of said jaws engaging with a distant end of the sample; moving the two jaws together so as to exert a force at each of said ends until the sample has completely broken; measuring the variations during the clamping on the basis of the time of the clamping force exerted at each end of the sample; determining the maximum value F
0 of said clamping force; marking three separate areas on the surface of one of the breaking surfaces, i.e. a first area close to the hole having a first type of embossment, a second area having a second type of embossment, and a third area having a third type of embossment that is less pronounced than the second type; measuring the distance L
0 between the edge of the hole and a transition line separating the second area from the third area; and calculating the parameter K
c on the basis of the force F
0 and distance L
0 .
公开/授权文献:
- EP2883033B1 PROCEDE DE MESURE DE LA TENACITE D'UN MATERIAU 公开/授权日:2016-09-07
IPC结构图谱:
G | 物理 |
--G01 | 测量;测试 |
----G01N | 借助于测定材料的化学或物理性质来测试或分析材料 |
------G01N3/00 | 用机械应力测试固体材料的强度特性 |
--------G01N3/60 | .测试材料,例如耐火材料耐急剧热变化的性能 |