EP2554259A4 HYDROISOMERIZATION CATALYST, METHOD FOR PRODUCING SAME, METHOD FOR DEWAXING HYDROCARBON OIL, METHOD FOR PRODUCING HYDROCARBON, AND METHOD FOR PRODUCING LUBRICANT BASE OIL
失效 - 权利终止

基本信息:
- 专利标题: HYDROISOMERIZATION CATALYST, METHOD FOR PRODUCING SAME, METHOD FOR DEWAXING HYDROCARBON OIL, METHOD FOR PRODUCING HYDROCARBON, AND METHOD FOR PRODUCING LUBRICANT BASE OIL
- 专利标题(中):加氢异构化工艺用于生产它,脱蜡油烃,工艺油气生产和方法,生产工艺的基础油
- 申请号:EP11762677 申请日:2011-03-24
- 公开(公告)号:EP2554259A4 公开(公告)日:2017-03-15
- 发明人: NAGAYASU YOSHIYUKI , HAYASAKA KAZUAKI , ONO HIDEKI , MATSUMOTO TAKAYA
- 申请人: JX NIPPON OIL & ENERGY CORP
- 专利权人: JX NIPPON OIL & ENERGY CORP
- 当前专利权人: JX NIPPON OIL & ENERGY CORP
- 优先权: JP2010075410 2010-03-29
- 主分类号: B01J29/74
- IPC分类号: B01J29/74 ; C10G45/64
摘要:
The hydroisomerization catalyst of the present invention is a catalyst used for hydroisomerization of a hydrocarbon, including a support including a calcined zeolite modified with at least one metal selected from the group consisting of Na, K, Cs, Mg, Ca, Ba, and K, and having a thermal history that includes heating at 350°C or more, and at least one inorganic oxide selected from the group consisting of alumina, silica, titania, boria, zirconia, magnesia, ceria, zinc oxide, phosphorus oxide, and a composite oxide containing a combination of at least two or more of these oxides; and at least one metal supported on the support and selected from the group consisting of elements belonging to Groups 8 to 10 of the periodic table, molybdenum and tungsten; wherein the zeolite is prepared from an ion-exchanged zeolite obtained by ion exchange of an organic template-containing zeolite containing an organic template and having a 10-membered ring one-dimensional porous structure in a solution containing ammonium ions and/or protons; and initial heating of the heating at 350°C or more of the thermal history experienced by the zeolite is conducted within the range of 350 to 450°C.
摘要(中):
本发明的加氢异构化催化剂用于烃的加氢异构化的催化剂,包括支撑包括与选自自由Na,K,铯,镁,钙,钡中选择的至少一种金属改性的煅烧沸石,和K 和具有热历史也包括加热在350℃以上,且选自氧化铝,二氧化硅,二氧化钛,氧化硼,氧化锆,氧化镁,二氧化铈,氧化锌,氧化磷中选出的至少一种无机氧化物,以及 复合氧化物含有至少两个或更多个本文氧化物的组合; 和至少一种金属负载于载体上和选自第VIII族周期表,钼和钨的10个元素的选择; worin沸石从在由含有有机模板的沸石含有有机模板的离子交换得到的离子交换沸石来制备,并且具有在溶液中有10元环的一维多孔结构含有铵离子和/或质子; 并且在由沸石所经历的热历史的350℃以上的加热的初始加热的350的范围内进行,以450℃
IPC结构图谱:
B | 作业;运输 |
--B01 | 一般的物理或化学的方法或装置 |
----B01J | 化学或物理方法,例如,催化作用、胶体化学;其有关设备 |
------B01J29/00 | 包含分子筛的催化剂 |
--------B01J29/03 | .不具有碱交换特性 |
----------B01J29/06 | ..硅铝酸盐 |
------------B01J29/08 | ...八面沸石型的,例如,X型或Y型的 |
--------------B01J29/72 | ....含铁族金属,贵金属或铜 |
----------------B01J29/74 | .....贵金属 |