基本信息:
- 专利标题: 复合焊连续焊接方法及装置、焊接成品、车体
- 专利标题(英):Hybrid welding continuous welding method and device, welding finished product and vehicle body
- 申请号:CN201910277678.7 申请日:2019-04-08
- 公开(公告)号:CN110000475A 公开(公告)日:2019-07-12
- 发明人: 韩晓辉 , 毛镇东 , 高月欣 , 郑凯 , 李刚卿
- 申请人: 中车青岛四方机车车辆股份有限公司
- 申请人地址: 山东省青岛市城阳区锦宏东路88号
- 专利权人: 中车青岛四方机车车辆股份有限公司
- 当前专利权人: 中车青岛四方机车车辆股份有限公司,青岛中车四方轨道装备科技有限公司
- 当前专利权人地址: 山东省青岛市城阳区锦宏东路88号
- 代理机构: 北京路浩知识产权代理有限公司
- 代理人: 苗青盛; 魏雪梅
- 主分类号: B23K26/348
- IPC分类号: B23K26/348 ; B23K26/70
The invention relates to the technical field of laser electrical arc welding, in particular to a hybrid welding continuous welding method and device, a welding finished product and a vehicle body. Thehybrid welding continuous welding method comprises carrying out hybrid welding on the groove of a weldment through laser and polarity-changing electric arc coupling, wherein the defocusing amount oflaser is less than the rayleigh range of laser. With adoption of the hybrid welding continuous welding method, the laser power density on the surface of the weldment is effectively reduced, the depth-to-width ratio of a welding seam is reduced, the diameter of a welding molten hole is increased, the hole of the welding molten hole caused by the small hole collapse phenomenon is effectively reducedto solve the problem in the prior art that the welding bubble is difficult to escape, generation of a hydrogen hole is reduced, the welding stability and reliability are effectively reduced, and themechanical property of the welding seam is improved.
公开/授权文献:
- CN110000475B 复合焊连续焊接方法及装置、焊接成品、车体 公开/授权日:2020-09-04
IPC结构图谱:
B | 作业;运输 |
--B23 | 机床;不包含在其他类目中的金属加工 |
----B23K | 钎焊或脱焊;焊接;用钎焊或焊接方法包覆或镀敷;局部加热切割,如火焰切割;用激光束加工 |
------B23K26/00 | 用激光束加工,例如焊接,切割,打孔 |
--------B23K26/20 | .连接,如焊接 |
----------B23K26/348 | ..与电弧加热结合的,例如TIG |