基本信息:
- 专利标题: 一种生物质炭/石墨烯柔性复合膜的制备方法
- 申请号:CN201710926638.1 申请日:2017-10-08
- 公开(公告)号:CN108538630B 公开(公告)日:2020-01-07
- 发明人: 徐斌 , 官亦标 , 吴琪 , 沈进冉 , 周淑琴 , 胡龙丰
- 申请人: 北京化工大学 , 中国电力科学研究院 , 国家电网公司 , 国网山东省电力公司青岛供电公司
- 申请人地址: 北京市朝阳区北三环东路15号
- 专利权人: 北京化工大学,中国电力科学研究院,国家电网公司,国网山东省电力公司青岛供电公司
- 当前专利权人: 北京化工大学,中国电力科学研究院,国家电网公司,国网山东省电力公司青岛供电公司
- 当前专利权人地址: 北京市朝阳区北三环东路15号
- 主分类号: H01G11/40
- IPC分类号: H01G11/40 ; H01G11/44 ; H01G11/86 ; H01M4/36 ; H01M4/587 ; H01M10/054
The invention provides a preparation method of a biomass charcoal/graphene flexible composite film. The nitrogen-rich biomass charcoal/graphene flexible composite film is prepared by the blended spinning solution containing the silk fibroin, the graphene oxide and the activator through the electrospinning technology and high temperature one-step carbonization activation. The material has the characteristics of being nitrogen-rich, porous and flexible. According to the method, the silk fibroin is rich in amino acids and can react with the graphene oxide in a cross-linking way through heating and stirring so that the graphene oxide is enabled to be aminated, the graphene oxide can be further reduced in the carbonization process, and the nitrogen atom part of the biomass residues in the composite material. The mass ratio of the biomass charcoal to the graphene in the obtained biomass charcoal/graphene flexible composite film is (0.5-9):1, the specific area is 1850-2740m2/g and the mitogencontent is 3.6-9.4%. The composite film is applied to the electrode material of the supercapacitor and the sodium ion battery so as to show high specific capacity, long cycle life and excellent rateperformance.
公开/授权文献:
- CN108538630A 一种生物质炭/石墨烯柔性复合膜的制备方法 公开/授权日:2018-09-14
IPC结构图谱:
H | 电学 |
--H01 | 基本电气元件 |
----H01G | 电容器;电解型的电容器、整流器、检波器、开关器件、光敏器件或热敏器件 |
------H01G11/00 | 混合电容器,即具有不同正极和负极的电容器;双电层(EDL)电容器;其制造方法或其零部件的制造方法 |
--------H01G11/10 | .多个混合或双电层电容器,如阵列或模块 |
----------H01G11/26 | ..以它们的结构为特征的,如多层、多孔或表面特征 |
------------H01G11/32 | ...碳基 |
--------------H01G11/40 | ....纤维 |