基本信息:
- 专利标题: 一种耐磨性斗齿的制作方法
- 专利标题(英):Manufacturing method for abrasion-resistant bucket teeth
- 申请号:CN201710514962.2 申请日:2017-06-29
- 公开(公告)号:CN107321889A 公开(公告)日:2017-11-07
- 发明人: 罗绍康
- 申请人: 宁波吉威熔模铸造有限公司
- 申请人地址: 浙江省宁波市鄞州区云龙镇荷花桥
- 专利权人: 宁波吉威熔模铸造有限公司
- 当前专利权人: 宁波吉威熔模铸造有限公司
- 当前专利权人地址: 浙江省宁波市鄞州区云龙镇荷花桥
- 代理机构: 余姚德盛专利代理事务所
- 代理人: 周积德
- 主分类号: B21J1/04
- IPC分类号: B21J1/04 ; B21J1/06 ; B21J5/02 ; C21D9/00 ; B24B9/04 ; B23P15/00
The invention discloses a manufacturing method for abrasion-resistant bucket teeth. The manufacturing method comprises the following steps that a bar is cut into sections, and the cut bar is placed on an automatic weighing device to be weighed; after weighed, the bar is fed into a heating furnace, heating treatment is conducted, and the bar is taken out of the furnace after heated; after heated, the bar is fed into a container under the forging temperature, and the container is used for calculating the mass and size of the bar in the unit; the container is conveyed into a pre-forging mold, pre-forging treatment is conducted, and the bar is fed into a finish forging mold after treatment, and finish forging forming is conducted; flanges of a semi-finished product are removed through polishing equipment; and the semi-finished product obtained after quenching treatment is conveyed into a tempering furnace, tempering insulation is conducted for 2 hours, then the product is taken out of the tempering furnace, and air cooling is conducted. Therefore, heat cutting is conducted directly under the forging temperature, cooling is not needed, time is saved, production efficiency is improved, thus product quality is ensured, in addition, the burr removing effect can be improved through the polishing equipment, and labor cost is reduced.
IPC结构图谱:
B | 作业;运输 |
--B21 | 基本上无切削的金属机械加工;金属冲压 |
----B21J | 锻造;锤击;压制;铆接;锻造炉 |
------B21J1/00 | 准备金属坯料 |
--------B21J1/04 | .通过锻压或压制仅进行初步成型 |