![一种改善预烧结工艺均热性的方法](/CN/2016/1/163/images/201610815549.jpg)
基本信息:
- 专利标题: 一种改善预烧结工艺均热性的方法
- 专利标题(英):Method for improving homo-heating property in pre-sintering process
- 申请号:CN201610815549.5 申请日:2016-09-12
- 公开(公告)号:CN106467934A 公开(公告)日:2017-03-01
- 发明人: 徐礼兵 , 周明顺 , 唐复平 , 翟立委 , 刘杰 , 张辉 , 姚林 , 王义栋 , 任子平 , 韩淑峰 , 宫作岩
- 申请人: 鞍钢股份有限公司
- 申请人地址: 辽宁省鞍山市铁西区鞍钢厂区内
- 专利权人: 鞍钢股份有限公司
- 当前专利权人: 鞍钢股份有限公司
- 当前专利权人地址: 辽宁省鞍山市铁西区鞍钢厂区内
- 主分类号: C22B1/16
- IPC分类号: C22B1/16
The invention provides a method for improving homo-heating property in a pre-sintering process. The method includes the steps of burdening, uniformly mixing of sintering materials, granulation, bottom material pavement, material distribution, ignition and sintering. During the sintering production process, a sintering mixture material is subjected to two-stage material distribution. Firstly, for the first time, a lower-layer sintering mixture material is distributed, material distribution thickness being 500-900 mm; and after ignition, the material is pre-sintered for a preset time, and then an upper-layer sintering mixture material is secondarily distributed on the surface of the material being sintered, material distribution thickness being 100-700 mm; and then ignition sintering is carried out again until sintering terminal, wherein the total thickness of the material layers is not less than 1000 mm; water content of the lower-layer sintering mixture material is controlled to be 5.9-6.7% and the water content of the upper-layer sintering mixture material is controlled to be 6.8-8.6%. By means of the method for sintering ore, quality is significantly improved and sintering solid fuel consumption is reduced, thus achieving the objects of homogenizing sintering, reducing cost and improving efficiency.
公开/授权文献:
- CN106467934B 一种改善预烧结工艺均热性的方法 公开/授权日:2018-12-04
IPC结构图谱:
C | 化学;冶金 |
--C22 | 冶金(铁的冶金入C21);黑色或有色金属合金;合金或有色金属的处理 |
----C22B | 金属的生产或精炼;原材料的预处理 |
------C22B1/00 | 矿石或废料的初步处理 |
--------C22B1/14 | .结块;制团;粘合;制粒 |
----------C22B1/16 | ..烧结;结块 |