基本信息:
- 专利标题: 一种煤焦油加氢改质催化剂及其制备方法
- 专利标题(英):Hydro-upgrading catalyst for coal tar and preparation method of catalyst
- 申请号:CN201510187542.9 申请日:2015-04-20
- 公开(公告)号:CN106140293A 公开(公告)日:2016-11-23
- 发明人: 闫琛洋 , 史雪君 , 杜少春 , 车中山 , 余海鹏 , 吴道洪
- 申请人: 北京神雾环境能源科技集团股份有限公司
- 申请人地址: 北京市昌平区马池口镇神牛路18号
- 专利权人: 北京神雾环境能源科技集团股份有限公司
- 当前专利权人: 神雾科技集团股份有限公司
- 当前专利权人地址: 北京市昌平区马池口镇神牛路18号
- 代理机构: 北京冠和权律师事务所
- 代理人: 朱健; 陈国军
- 主分类号: B01J29/85
- IPC分类号: B01J29/85 ; C10G45/12 ; C10G45/54 ; C10G49/08
The invention discloses a hydro-upgrading catalyst for coal tar and a preparation method of the catalyst. The catalyst is prepared from an active metal component, a catalyst promoter component and a carrier, wherein the active metal component is selected from one or more metal elements of Ni, Mo, Co and W, the catalyst promoter component is P2O5 or is selected from one or more metal elements of Fe and Mn, and the carrier is phosphoric acid modified kaolin; the weight of the active metal component is 10%-30% of that of the carrier on the basis of oxide, the weight of metal elements in the catalyst promoter component is 3%-7% of that of the carrier on the basis of oxide, and the dosage of phosphoric acid is 1%-4% of the weight of the carrier. The hydro-upgrading catalyst not only has good hydrogen desulfurization, denitrification and colloid removal activity, but also has higher aromatics saturation and ring opening capability.
IPC结构图谱:
B | 作业;运输 |
--B01 | 一般的物理或化学的方法或装置 |
----B01J | 化学或物理方法,例如,催化作用、胶体化学;其有关设备 |
------B01J29/00 | 包含分子筛的催化剂 |
--------B01J29/03 | .不具有碱交换特性 |
----------B01J29/84 | ..含其他元素,如金属、硼的磷铝酸盐 |
------------B01J29/85 | ...磷硅铝酸盐 |